Method for manufacturing semiconductor device

2Forward Citations (#43531550 Global)
0.1/yrCitation Velocity (#41835006 Global)
0.93Citation PageRank (#46129777 Global)
21Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A substrate is exposed to a plasma generated from a gas containing an impurity, thereby doping a surface portion of the substrate with the impurity and thus forming an impurity region. A predetermined plasma doping time is used, which is included within a time range over which a deposition rate on the substrate by the plasma is greater than 0 nm/min and less than or equal to 5 nm/min.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a semiconductor device, comprising: forming an impurity region by exposing a substrate to a plasma generated from a gas containing an impurity to thereby dope a surface portion of the substrate with the impurity, wherein the method uses a predetermined plasma doping time included within a time range over which a deposition rate of a film containing the impurity and deposited on the substrate by the plasma is greater than 0 nm/min and less than or equal to 5 nm/min.

  2. Claim 2Depends on #1

    The method for manufacturing a semiconductor device of claim 1 , wherein the deposition rate on the substrate by the plasma is greater than 0 nm/min and less than or equal to 2 nm/min within the time range.

  3. Claim 3Depends on #1

    The method for manufacturing a semiconductor device of claim 1 , wherein the time range is a range of 50 seconds or more and 200 seconds or

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
US 4,496,450 AProcess for the production of a multicomponent thin film198523
US 4,696,883 AMember having light receiving layer with smoothly connected non-parallel interfaces and surface reflective layer19873
JP S6461020 APlasma ion doping method—4
US 6,403,410 B1Plasma doping system and plasma doping method200231
WO 02,084,724 A1Method for surface treatment and system for fabricating semiconductor device—12
US 2003153101 A1Method for surface treatment and system for fabricating semiconductor device—24
WO 2005/034221 A1Substrate and its production method—7
US 2006099830 A1Plasma implantation using halogenated dopant species to limit deposition of surface layers—107
WO 2006/064772 A1Plasma doping method—22
WO 2006/121131 A1Plasma doping method and plasma doping apparatus—18
US 7,192,854 B2Method of plasma doping200717
US 2007111548 A1Plasma doping method and plasma doping apparatus—8
US 2007176124 A1Plasma doping method and plasma doping apparatus—16
US 2008067439 A1Plasma doping method and plasma doping apparatus—2
US 7,348,264 B2Plasma doping method200815
US 2008233723 A1Plasma doping method and apparatus—17
US 2008258082 A1Plasma Processing Method and Plasma Processing Apparatus—8
US 2009042321 A1Apparatus and method for plasma doping—34
US 2009227096 A1Method Of Forming A Retrograde Material Profile Using Ion Implantation—14
US 2010009469 A1Plasma doping method and apparatus—11
US 7,759,254 B2Method for forming impurity-introduced layer, method for cleaning object to be processed apparatus for introducing impurity and method for producing device201018

Non-Patent Literature (5)

  • D. Lenoble, "Advanced junction fabrication challenges at the 45nm node," Semiconductor Fabtech-30th Edition, pp. 114-130.
  • Shu Qin et al., "Device Performance Evaluation of PMOS Devices Fabricated by B2H6 PIII/PLAD Process of Poly-Si Gate Doping," International Workshop in Junction Technology, pp. 68, 2006.
  • Y, Sasaki et al., "B2H6 Plasma Doping with 'In-situ He Pre-amorphization,'" 2004 Symposium on VLSI Technology, p. 180-181.
  • Y. Sasaki et al., "New method of Plasma doping with in-situ Helium pre-amorphization," Nuclear instruments and Methods in Physics Research B 237 (2005) pp. 41-45.
  • Y. Sasaki et al., "Production-Worth USJ Formation by Self-Regulatory Plasma Doping Method," CP866 Ion Implantation Technology, 2006 American Institute of Physics, pp. 524-527.