Varied impurity profile region formation for varying breakdown voltage of devices
Abstract
Methods are disclosed for forming a varied impurity profile for a collector using scattered ions while simultaneously forming a subcollector. In one embodiment, the invention includes: providing a substrate; forming a mask layer on the substrate including a first opening having a first dimension; and substantially simultaneously forming through the first opening a first impurity region at a first depth in the substrate (subcollector) and a second impurity region at a second depth different than the first depth in the substrate. The breakdown voltage of a device can be controlled by the size of the first dimension, i.e., the distance of first opening to an active region of the device. Numerous different sized openings can be used to provide devices with different breakdown voltages using a single mask and single implant. A semiconductor device is also disclosed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 32 · Forward citations: 0.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method, comprising: providing a substrate; forming a mask layer on the substrate including a first opening having a first dimension; and substantially simultaneously forming through the first opening a first subcollector having a first impurity at a first depth in the substrate and a first collector having a second impurity at a second depth different from the first depth in the substrate, wherein an impurity profile of the second impurity that is within the first collector comprises a high impurity concentration of the second impurity that extends from near center of the first collector to
- Claim 2Depends on #1
The method of claim 1 , wherein the formi
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (32)
Non-Patent Literature (5)
- Brack, K. et al., "Lateral Nonuniform Doping of Semiconductor Structures by Ion Implantation," IBM Technical Disclosure Bulletin, vol. 16, No. 10, Mar. 1974, pp. 3287-3288.
- Coolbaugh et al., U.S. Appl. No. 10/908,884, filed May 31, 2005, Office Action Summary, Apr. 17, 2007, 7 pages.
- Coolbaugh et al., U.S. Appl. No. 10/908,884, filed May 31, 2005, Office Action Summary, Dec. 8, 2006, 10 pages.
- Coolbaugh et al., U.S. Appl. No. 10/908,884, filed May 31, 2005, Office Action Summary, Jan. 28, 2008, 11 pages.
- Coolbaugh et al., U.S. Appl. No. 10/908,884, filed May 31, 2005, Office Action Summary, Jul. 23, 2008, 10 pages.