US 8,026,459 B2#17354962 Most CitedActiveUnited States (USPTO)Utility

Laser surface treatment

6Forward Citations (#17354962 Global)
0.4/yrCitation Velocity (#19742913 Global)
1.75Citation PageRank (#18021860 Global)
25Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A laser surface treatment for reducing reflection loss on the surface of an optical material is provided. A metal film is formed on the surface of the optical material, and then the metal film is removed from the optical material by irradiation of an ultra-intense short-pulse laser beam having a pulse width of 1 femtosecond to 100 picoseconds, so that a fine periodic structure is formed on the surface of the optical material exposed by the removal of the metal film. The obtained fine periodic structure has asperities with a periodic interval of preferably 50 to 1000 nm, which can be controlled by changing the laser energy density.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 6.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process of developing a periodic structure in a surface of an optical transparent substrate, said process comprising the steps of: forming a metal film having a thickness of 50 nm to 1000 nm on a surface of said optical transparent substrate made of non-metal material; and irradiating an ultra-intense short-pulse laser beam having a pulse width of 1 femtosecond (fs) to 100 picoseconds (ps) to said metal film in order to ablate a portion of said metal film to generate within an ablated portion of said metal film, a resulting metal plasma, which interacts with said laser beam for etching the s

  2. Claim 2Depends on #1

    The process of developing a periodic structure in a surface of an optical transparent substrate as set forth in claim 1 , wherein said ul

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (25)

PatentTitleYearCitations
US 5,072,091 AMethod and apparatus for metal surface process by laser beam199152
JP H06198466 ARainbow color development processing method—6
JP H06212451 AMethod for ornamenting metallic surface—25
US 5,417,896 APreparation of sheet-like polyethylene terephthalate materials having little surface roughness199515
US 5,558,789 AMethod of applying a laser beam creating micro-scale surface structures prior to deposition of film for increased adhesion199690
US 5,910,256 AMethod for manufacturing a diffraction type optical element199927
WO 0,030,166 A1Method for producing nanostructures in thin films—2
US 6,291,797 B1Laser machining method for glass substrate, diffraction type optical device fabricated by the machining method, and method of manufacturing optical device200115
US 2002097962 A1Single and multilayer waveguides and fabrication process—406
JP 2002372641 AMethod for manufacturing optical waveguide, optical waveguide and wavelength conversion device—13
JP 2003057422 AMethod for forming cyclic microstructure by femtosecond laser irradiation—46
US 6,555,781 B2Ultrashort pulsed laser micromachining/submicromachining using an acoustooptic scanning device with dispersion compensation200356
JP 2003133690 AMethod for forming circuit by using ultra short pulse laser—28
US 2003185697 A1Method of making sintered object—16
US 6,657,155 B2Method of and apparatus for making a three-dimensional object200350
US 2004013805 A1Processing method of creating rainbow color, method of manufacturing article which presents rainbow-colored reflective luster, and article which presents rainbow-coloured reflective luster—26
US 6,682,688 B1Method of manufacturing a three-dimensional object200466
US 2004149705 A1Method and apparatus for processing three-dimensional structure, method for producing three-dimensional shape product and three-dimensional structure—18
US 2004182201 A1Metal powder composition for use in selective laser sintering—28
US 2004228754 A1Method of making a three-dimensional sintered product—47
JP 2004339538 AMicro-bump production method, fine-mesh production method, laser machining device, and substrate for production—7
JP 2004354535 AMethod for processing light receiving/emitting part of optical medium—5
JP 2004360012 AMethod and device for surface treatment of close-contact metal surface—10
US 2005029711 A1Method of making three-dimensional object—21

Non-Patent Literature (5)

  • Blaesi et al., "Entspiegeln Mit Mottenaugenstrukturen Spritzgiessen Funktionaler Mikrostrukturierter Oberflaechen" Kunstsoffe, Carl Hanser Verlag, Munchen, vol. 92, No. 5: 50-53 (2002).
  • Choi et al., "Formation of Nano-Pattern on Metal Using Femtosecond Laser Pulses" Hankook Kwanghak Hoeji Opt. Soc. Korea, vol. 17, No. 2: 203-206 (2006), abstract only.
  • English Language Abstract of JP 2003-057422.
  • English Language Abstract of JP 2004-360012.
  • Japanese Office Action dated Jul. 27, 2010 that issued with respect to Japanese Patent Application No. 2005-093145, along with a partial English language translation.