Patents
US 8,018,682 B2#27263841 Most CitedActiveUnited States (USPTO)Utility

Magnetic disk comprising an aluminum alloy oxynitride underlayer and a diamond-like carbon overcoat

4Forward Citations (#27263841 Global)
0.3/yrCitation Velocity (#27798972 Global)
1.06Citation PageRank (#38502997 Global)
24Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A magnetic disk is protected by a bilayer. The bilayer is formed as an adhesion enhancing underlayer and a protective diamond-like carbon (DLC) overlayer. The underlayer is formed of an aluminum or alloyed aluminum oxynitride, having the general formula AlO x N y or Me z AlO x N y where Me z symbolizes Ti z , Si z or Cr z and where x, y and z can be varied within the formation process. By adjusting the values of x and y the adhesion underlayer contributes to such qualities of the protective bilayer as stress compensation, chemical and mechanical stability and low electrical conductivity. Various methods of forming the underlayer are provided, including reactive ion sputtering, plasma assisted chemical vapor deposition, pulsed laser deposition and plasma immersion ion implantation.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A surface-protected magnetic disk comprising: the magnetic disk; a surface-protecting bilayer formed on the disk, the bilayer comprising: an adhesion enhancing underlayer formed of an aluminum oxynitride, AlO x N y , formed on said disk; and a DLC overlayer formed on said underlayer.

  2. Claim 2Depends on #1

    The surface-protected magnetic disk of claim 1 wherein x is in the range between approximately 0 and 1.5 and y is in the range between approximately 0 and 1.

  3. Claim 3Depends on #1

    The surface-protected magnetic disk of claim 1 wherein said underlayer is formed to a thickness less than approximately 50 angstroms.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
US 4,861,669 ASputtered titanium oxynitride films1989182
JP H02182880 ACoating film made of carbon or having carbon as main component via buffer layer and production thereof—7
US 4,952,904 AAdhesion layer for platinum based sensors199098
JP H02215522 AComposite laminated film—4
JP H03195301 AAccident diagnosis method for motorcar—4
US 5,070,036 AProcess for contacting and interconnecting semiconductor devices within an integrated circuit199155
JP H04235283 AApparatus and method for forming coating film—10
US 5,227,196 AMethod of forming a carbon film on a substrate made of an oxide material199332
US 5,567,523 AMagnetic recording medium comprising a carbon substrate, a silicon or aluminum nitride sub layer, and a barium hexaferrite magnetic layer199660
US 5,609,948 ALaminate containing diamond-like carbon and thin-film magnetic head assembly formed thereon199744
DE 19,730,884 A1Chromium oxynitride sputter deposition from pure chromium target—8
JP H11268164 ABase material with carbon film—4
US 6,238,803 B1Titanium nitride barrier layers200120
JP 3,195,301 B2炭素系被膜を有する基材20014
US 6,296,742 B1Method and apparatus for magnetically enhanced sputtering2001120
US 6,517,956 B1Magneto-resistance recording media comprising aluminum nitride corrosion barrier layer and a c-overcoat200314
US 6,569,295 B2Method for grading surface topography for improved step coverage and planarization200315
US 6,915,796 B2Superabrasive wire saw and associated methods of manufacture200541
US 7,091,541 B2Semiconductor device using a conductive film and method of manufacturing the same200617
US 7,300,556 B2Method for depositing a thin film adhesion layer20074
US 7,465,378 B2Method for reactive sputtering deposition20084
JP 4,235,283 B2小三本鎖形成pnaオリゴ20094
US 7,722,968 B2Magnetic disk and manufacturing method thereof20104
US 7,881,013 B2Recording tape cartridge20117

Non-Patent Literature (5)

  • "Control of reactive sputtering processes," by W.D. Sproul et al., Thin Solid Films 491 (2005) 1-17, 2005 Elsevier B. V., doi: 10.1016/j.tsf.2005.02.022.
  • "Growth dynamics of aluminum nitride and aluminum oxide thin films synthesized by ion-assisted deposition," by R. P. Netterfield et al., Journal of Applied Physics vol. 63, No. 3, Feb. 1, 1988, pp. 760-769, 1988 American Institute of Physics.
  • "Reaction of N2 beams with aluminum surfaces," by J. Ahley Taylor et al., Journal of Che. Phys. vol. 75, No. 4, Aug. 14, 1981, pp. 1735-1745, 1981 American Institute of Physics.
  • "Reactive ion assisted deposition of aluminum oxynitride thin films," by Chang Kwon Hwangbo et al., Jul. 15, 1989, vol. 28, No. 14, Applied Optics, pp. 2779-2784.
  • Handbook of Plasma Immersion Ion Implantation and Deposition, Edited by Andre Anders, Copyright 2000, John Wiley & Sons, Inc. NY, 20 pages.