Poly(arylene ether)-polysiloxane composition and method

97Forward Citations (#254843 Global)
6.5/yrCitation Velocity (#148897 Global)
8.19Citation PageRank (#1476023 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A thermoplastic composition includes a poly(arylene ether) and a poly(arylene ether)-polysiloxane block copolymer. The thermoplastic composition is prepared by a method that includes oxidatively copolymerizing a monohydric phenol and a hydroxyaryl-terminated polysiloxane. The method is simpler than prior methods of preparing poly(arylene ether)-polysiloxane block copolymers by linking pre-formed poly(arylene ether) and polysiloxane blocks. The method is also produces greater incorporation of polysiloxane into the poly(arylene ether)-polysiloxane block copolymer than prior methods of copolymerizing monohydric phenols and hydroxyaryl-terminated polysiloxane.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 97.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of preparing a thermoplastic composition, comprising: oxidatively copolymerizing a monohydric phenol and a hydroxyaryl-terminated polysiloxane to form a thermoplastic composition; wherein the oxidative copolymerization is initiated in the presence of at least 50 weight percent of the hydroxyaryl-terminated polysiloxane and less than or equal to 50 weight percent of the monohydric phenol; wherein the oxidative copolymerization is conducted with a reaction time greater than or equal to 110 minutes; wherein the hydroxyaryl-terminated polysiloxane comprises, on average, 35 to 80 siloxane

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 97 total)

PatentTitleYearCitations
US 10,407,546 B2Acrylate-terminated urethane polybutadienes from low-monomer 1:1 monoadducts from reactive olefinic compounds and diisocyanates and hydroxy-terminated polybutadienes for liquid optically clear adhesives (LOCAs)20192
US 8,933,155 B2Reinforced poly(phenylene ether)-polysiloxane block copolymer composition, and article comprising same20153
US 9,187,639 B2Thermal plastic blends with improved impact strength and flow20156
EP 3,677,646 A1Thermoplastic composition, method for the manufacture thereof, and articles including the thermoplastic composition—0
WO 2014/195874 A1Blended thermoplastic compositions with improved impact strength and flow—3
WO 2018/013388 A1Foamed thermoplastic material, method for the manufacture thereof, articles prepared therefrom, and article-forming method—2
WO 2014/033665 A1Glass-filled polyamide composition and article—2
WO 2016/120682 A1Flame retardant poly(arylene ether)/polystyrene foamed material and associated method of making and article—1
EP 4,574,902 A1Electrostatically paintable molded articles and method for the manufacture thereof—0
EP 4,382,289 A1Laminated foam article and associated method and electric vehicle battery pack—0
US 8,552,095 B1Flame-retardant polymer composition and article20134
US 9,944,768 B2High modulus laser direct structuring polycarbonate composites with enhanced plating performance and broad laser window and methods for the manufacture and use thereof20180
WO 2014/152107 A1Blended polymer compositions with improved mold release properties—9
US 10,290,389 B2Thermoplastic compositions containing nanoscale-sized particle additives for laser direct structuring and methods for the manufacture and use thereof20190
WO 2020/005544 A1Thermoplastic composition, method for the manufacture thereof, and articles prepared therefrom—3

Non-Patent Literature (5)

  • Ablemarle, Saytex HP-3010 Flame Retardant, Feb. 2008, 2 pages.
  • ASTM D 2240-05, "Standard Test Method for Rubber Property-Durometer Hardness".
  • ASTM D 2240-05, "Standard Test Method for Rubber Property—Durometer Hardness".
  • ASTM D 3763-08, Standard Test Method for High Speed Puncture Properties of Plastics Using Load and Displacement Sensors, Downloaded Jul. 12, 2010, 9 pages.
  • ASTM D 648-07, Standard Test Method for Deflection Temperature of Plastics Under Flexural Load in the Edgewise Position, Downloaded Jan. 12, 2009, 13 pages.