Polymer-cement composites and methods of making same

1Forward Citations (#49748717 Global)
0.1/yrCitation Velocity (#50725339 Global)
0.88Citation PageRank (#49265406 Global)
30Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A polymer-cement composite comprises, by weight percent, about 40% to 50% inert, inorganic filler material, such as silica sand; about 12% to 23% latex, preferably in aqueous suspension; about 20% to 25% hydraulic cement; and reactive silica in an amount of at least about 6 weight percent. The reactive silica is a pozzolanic material, and in preferred embodiments, where the cement is portland cement, comprises an advantageous mixture of precipitated and ground silica. All solid components have a particle size of less than about 300 microns. The polymer-cement composite is preferably made by dry mixing of the powdered components throughly in a high intensity mixer, adding the liquid components, and wet mixing to form a thoroughly blended, de-aired green mixture. The green mixture is formed into any desired shape, cured, and dried. Preferably, the product is cured in a warm, moist environment.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 30 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A polymer-cement composite comprising: about 12 to about 23 weight percent latex, the latex including polymer solids and water; about 20 to about 25 weight percent portland cement, the cement being present in an amount sufficient to provide a weight ratio of water to cement of up to about 0.49 and a ratio of latex polymer solids to cement (ls/c) of between 0.3 and 0.6, calcium hydroxide being produced when the cement is hydrated with water; filler in an amount sufficient to provide a weight ratio of filler to cement of about 1.90 to about 2.10; and about 6 to about 15 weight percent reactive s

  2. Claim 2Depends on #1

    The polymer-cement composite of claim 1 wherein the latex comprises an aqueous suspension.

  3. Claim 3Depends on #2

    The polymer-cement composite of claim 2 wherein the latex comprises an aqueous suspension of styrene-but

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (30)

PatentTitleYearCitations
DE 2,749,432 A1Verfahren zur herstellung von zementprodukten—2
EP 0,069,586 A2Polymer-modified cement mortars and concretes and processes for the production thereof—18
EP 0,173,553 A1Lightweight concrete roof tiles—6
GB 2,192,392 AImprovement in concrete articles—15
WO 8,901,918 A1Lightweight concrete roof tiles and similar products—8
US 4,849,018 AUtilization of latexes with aluminous cement and gypsum composition198950
US 4,861,822 ALatexes as binders for cast ceiling tiles198944
US 4,880,467 ACementitious dough or paste comprising at least one hydraulic element and at least one polymer latex198940
EP 0,347,092 A2Process for the production of concrete building products—27
US 5,075,358 AMultiple purpose patching composition199135
US 5,185,389 ALatex modified mortar and concrete199349
US 5,192,366 ACement admixture and cement composition199344
GB 2,262,521 ACementitious material—11
US 5,268,028 ALightweight concrete roof tiles and similar products199329
US 5,269,845 ACalcium aluminate composition and process for making same199344
US 5,332,774 APolyvinyl acetal resins based on hydroxyaldehydes and use of the resins in laminar structures199438
WO 9,424,062 A1Lightweight concrete roof tiles—10
US 5,362,320 ASandable low shrinkage mortar patching/coating compound199417
US 5,366,550 ALatex modified cement-based thin set adhesive199435
FR 2,705,663 A1Sand concrete of high tensile strength and articles, especially thin plates intended for the building industry, made of such a sand concrete and process for the manufacture of these articles—6
US 5,476,343 AOffshore pipeline insulated with a cementitious coating199530
US 5,496,404 AProcess of recycling paint waste199621
US 5,565,027 ACement composition199610
US 5,594,050 ACement composition containing chemically crosslinked polyvinyl alcohol (PVA)199723
US 5,603,758 AComposition useful for lightweight roof tiles and method of producing said composition199748
US 5,668,844 ASelf-calibrated tomosynthetic, radiographic-imaging system, method, and device199771
US 5,795,924 AResilient well cement compositions and methods199883
US 5,891,374 AMethod of making extruded fiber reinforced cement matrix composites199949
WO 0,056,679 A1Polymer-cement composites and methods of making same—9

Non-Patent Literature (5)

  • Ramakrishnan, National Cooperative Highway Research Program Synthesis of Highway Practice 179:: Latex Modified Concretes and Mortars, Transportation Research Board, National Research Council (Washington: 1992). Relevant Pages: p. 1 (paragraphs 1-4), 2-5, 11-12, 13-14 (including tables 9 &11).
  • REMR Material Data Sheet CM-LA-1.1 Latex Admixture for Portland-Cement Concrete and Mortar: Polyvinyl NeoCryl A-1055. Date: 1987.
  • REMR Material Data Sheet CM-LA-1.2 Latex Admixture for Portland-Cement Concrete and Mortar: AKKRO 7-T. Date: 1987.
  • REMR Material Data Sheet CM-LA-1.3 latex admixture for Portland-Cement Concrete and Mortar: ACRYL 60. Date: 1987.
  • REMR Material Data Sheet CM-LA-1.4 Latex Admixture for Portland-Cement Concrete and Mortar: ACRYL-Set. Date: 1994.