Patents
US 8,017,182 B2#8610236 Most CitedActiveUnited States (USPTO)Utility

Method for depositing thin films by mixed pulsed CVD and ALD

12Forward Citations (#8610236 Global)
0.8/yrCitation Velocity (#9186570 Global)
1.90Citation PageRank (#15706830 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Films are deposited on a substrate by a process in which atomic layer deposition (ALD) is used to deposit one layer of the film and pulsed chemical vapor deposition (CVD) is used to deposit another layer of the film. During the ALD part of the process, a layer is formed by flowing sequential and alternating pulses of mutually reactive reactants that deposit self-limitingly on a substrate. During the pulsed CVD part of the process, another layer is deposited by flowing two CVD reactants into a reaction chamber, with at least a first of the CVD reactants flowed into the reaction chamber in pulses, with those pulses overlapping at least partially with the flow of a second of the CVD reactants. The ALD and CVD parts of the process ca be used to deposit layers with different compositions, thereby forming, e.g., nanolaminate films. Preferably, high quality layers are formed by flowing the second CVD reactant into the reaction chamber for a longer total duration than the first CVD reactant. In some embodiments, the pulses of the third reactant at separated by a duration at least about 1.75 times the length of the pulse. Preferably, less than about 8 monolayers of material are deposited pe

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 12.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for depositing a multi-component thin film on a substrate in a reaction chamber, the method comprising: performing a plurality of deposition cycles, each cycle comprising: depositing a first component of the film on the substrate by flowing a first and second reactant into the reaction chamber in sequential and alternating pulses during a period A, the first and second reactants depositing self-limitedly on the substrate, wherein the first component is an oxide; and depositing a second component of the film by flowing a third reactant into the reaction chamber while simultaneously flo

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,058,430 AMethod for producing compound thin films19771,251
US 4,927,670 AChemical vapor deposition of mixed metal oxide coatings1990137
US 5,208,069 AMethod for passivating the inner surface by deposition of a ceramic coating of an apparatus subject to coking, apparatus prepared thereby, and method of utilizing apparatus prepared thereby199373
US 5,246,881 ALow-pressure chemical vapor deposition process for depositing high-density, highly-conformal, titanium nitride films of low bulk resistivity1993139
US 5,279,857 AProcess for forming low resistivity titanium nitride films199442
US 5,342,652 AMethod of nucleating tungsten on titanium nitride by CVD without silane1994112
JP H08264530 AMethod and system for fabricating semiconductor device—72
US 5,595,784 ATitanium nitride and multilayers formed by chemical vapor deposition of titanium halides1997111
US 5,691,235 AMethod of depositing tungsten nitride using a source gas comprising silicon1997113
US 5,711,811 AMethod and equipment for growing thin films1998575
US 5,723,384 AMethod for manufacturing a capacitor in a semiconductor device using selective tungsten nitride thin film199889
EP 0,899,779 A2Method for fabricating thermally stable contacts—43
US 5,916,365 ASequential chemical vapor deposition1999819
US 6,015,590 AMethod for growing thin films2000414
US 6,087,257 AMethods of fabricating a selectively deposited tungsten nitride layer and metal wiring using a tungsten nitride layer200051
WO 0,047,404 A1Chemical vapor deposition of tungsten nitride—25
WO 0,054,320 A1Radical-assisted sequential cvd—88
US 6,203,613 B1Atomic layer deposition with nitrate containing precursors2001824

Non-Patent Literature (5)

  • Andricacos, et al., "Damascene copper electroplating for chip," IBM Jour. Research and Dev., 42:567 (1998).
  • Elers, et al., "NbC15 as a precursor in atomic layer epitaxy," Applied Surface Science, 82/83:468-474 (1994).
  • Engbrecht, E.R., et al., "Chemical Vapor Deposition Growth and Properties of TaCxNy." Thin Solid Films 418 (2002) pp. 145-150.
  • Hiltunen, et al., "Nitrides to titanium, niobium, tantalum and molybdenum grown as thin films by the atomic layer epitaxy method," Thin Solid Films, 166:149-154 (1988).
  • Kim, Jin-Hyock, et al., "Film growth model of atomic layer deposition for multicomponent thin films". Journal of Applied Physics 97, 093505-1 to 093505-5 (2005).