Method for optimizing direct wafer bond line width for reduction of parasitic capacitance in MEMS accelerometers
Abstract
A method for optimizing direct wafer bond line width for reduction of parasitic capacitance in a MEMS device by reducing the width of a bond line between a first and a second wafer, exposing the MEMS device to a water vapor for a predetermined time period and at a first temperature capable of evaporating water, cooling the MEMS device at a second temperature capable of freezing the water, and operating the MEMS device at a third temperature capable of freezing the water to determine if there is discontinuity during operation.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for testing wafer bond line width in a MEMS device, the MEMS device having at least a first and second wafer layer with a bond line between each wafer layer, the method comprising the steps of: exposing the MEMS device to a vaporized fluid for a predetermined time period at a first temperature, within a range of temperatures for evaporating the fluid; cooling the MEMS device to a second temperature, within a range of temperatures for freezing the fluid; testing the MEMS device by operating the device at a third temperature, within a range of temperatures for freezing the fluid, to det
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗