Abstract

A method for producing a tungsten trioxide powder for a photocatalyst according to the present invention is characterized by comprising a sublimation step for obtaining a tungsten trioxide powder by subliming a tungsten metal powder or a tungsten compound powder by using inductively coupled plasma process in an oxygen atmosphere, and a heat treatment step for heat-treating the tungsten trioxide powder obtained in the sublimation step at 300° C. to 1000° C. for 10 minutes to 2 hours in an oxidizing atmosphere. A tungsten trioxide powder which is obtained by the method for producing a tungsten trioxide powder for a photocatalyst according to the present invention has excellent photocatalytic performance under visible light.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 9.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for producing a tungsten trioxide powder comprising: subliming a tungsten metal powder or a tungsten compound powder by at least one of the following processes in an oxygen atmosphere to produce a tungsten oxide powder: an inductively coupled plasma process, an arc discharge process, a laser process, and an electron beam process; and heat-treating the tungsten oxide powder at 300° C. to 1000° C. for 10 minutes to 2 hours in an oxidizing atmosphere to provide the tungsten trioxide powder.

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the tungsten metal powder or the tungsten compound powder has an average particle size of 0.1 μm to 100 μm.

  3. Claim 3Depends on #1

    The method according to claim 1 , wherein the sublimation in the oxygen atmosphere is achieved by an inductively coupled plasma process and the tungsten metal powder or the tungsten co

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (19)

PatentTitleYearCitations
JP S61242902 AProduction of ultrafine particle of high-melting metallic oxide—15
JP H026339 AProduction of ultrafine particle of tungsten or tungsten oxide—29
JP H0437610 AHyperfine tungsten oxide particles—5
US 5,613,998 AReclamation process for tungsten carbide and tungsten-based materials199712
JP H09249542 AUltraviolet light screening agent and preparation for external use for skin having ultraviolet light screening effect—13
US 5,984,997 ACombustion of emulsions: A method and process for producing fine powders1999178
JP 2001152130 APhotocatalytically hydrophilizable member and its manufacturing method—24
US 2002016250 A1Method for photocatalytically rendering a surface of a substrate superhydrophilic, a substrate with a superhydrophilic photocatalytic surface, and method of making thereof—75
JP 2002293544 ATungsten oxide fine particle and method for producing the same—23
US 6,832,735 B2Post-processed nanoscale powders and method for such post-processing200435
US 6,841,142 B1Bulk synthesis of long nanotubes of transition metal chalcogenides200523
US 2005025700 A1Preparation of tungsten oxide—49
JP 2006102737 AFine particle manufacturing method—24
US 2007177372 A1Photocatalytic material, photocatalyst, photocatalytic product, lighting apparatus, and method of producing photocatalytic material—29
WO 2007/088891 A1Photocatalyst material and, containing the same, photocatalyst composition and photocatalyst product—14
US 2009023583 A1Photocatalyst material, photocatalyst composition using the same and photocatalyst product—17
US 2010204041 A1Visible-light-responsive photocatalyst powder, and visible-light-responsive photocatalytic material, photocatalytic coating material and photocatalytic product each using the same—9
US 2010204040 A1Visible-light-responsive photocatalyst powder, method of manufacturing the same, and visible-light-responsive photocatalytic material, photocatalytic coating material and photocatalytic product each using the same—10
US 2010292075 A1Visible light response-type photocatalyst powder, visible light response-type photocatalyst material using the visible light response-type photocatalyst powder, photocatalyst coating material, and photocatalyst product—15

Non-Patent Literature (5)

  • "Nanocrystalline tungsten oxide thick-films with high sensitivity to H2S at room temperature," J. L. Solis et al. Sensors and Actuators B 77 (2001), pp. 316-321.
  • "Oxygen partial pressure effect on the preparation of nanocrystalline tungsten oxide powders by a plasma arc gas condensation technique," Cherng-Yuh Su et al. International Journal of Refractory Metals and Hard Materials 26 (2008), pp. 423-428.
  • "Preparation and characterization of doped WO3 photocatalyst powders," M. Ashokkumar et al. Journal of Materials Science Letters 24 (1989), pp. 2135-2139.
  • "Preparation of metal oxide particles by an arc plasma method," O. K. Ozawa et al. Annual Meeting of the Ceramic Society of Japan, Mar. 22, 2003, p. 40.
  • "Production of photo-catalyst TiO2 and high-temperature phase WO3 ultra-fine particles by DC arc discharge," Y. Guo et al. Journal of Crystal Growth 275 (2005), pp. e2031-e2036.