Method of making heat treated coated article using diamond-like carbon (DLC) coating and protective film

5Forward Citations (#22272434 Global)
0.3/yrCitation Velocity (#23238687 Global)
1.20Citation PageRank (#32261929 Global)
46Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

There is provided a method of making a heat treated (HT) coated article to be used in shower door applications, window applications, or any other suitable applications where transparent coated articles are desired. The method may include heat treating a glass substrate coated with at least a layer of or including diamond-like carbon (DLC) or other type of carbon, with a protective film thereon. In certain example embodiments, the protective film may be of or include a layer of or including SnO x prior to HT. Optionally, a release layer of a material such as zinc oxide may be provided between the SnO x and the DLC. Following and/or during heat treatment the SnO x transforms into SnO y (y>x) so that stress is created due to the SnO x to SnO y transition. Then, during quenching, stress relief may occur which causes the layer to buckle, creating cracks which may act as liquid channels that permit the sacrificial film to be easily removed via washing or the like.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 46 · Forward citations: 5.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of making a heat treated coated article, the method comprising: providing a glass substrate; forming at least a layer comprising carbon on the glass substrate; forming a protective film on the glass substrate over at least the layer comprising carbon, the protective film including a layer comprising SnO x , where x is from about 0.75 to 1.5, and a layer comprising substoichiometric zinc oxide ZnO t where t is from 0.1 to 0.8, wherein in the protective film the layer comprising zinc oxide ZnO t is located between and contacting the layer comprising carbon and the layer comprising SnO

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (46)

PatentTitleYearCitations
US 4,715,879 AMethod for the manufacture of a tempered and/or curved glass pane with reduced transmission198792
US 5,073,450 ALaminated glazing unit199137
US 5,135,808 AAbrasion wear resistant coated substrate product1992241
US 5,229,194 AHeat treatable sputter-coated glass systems1993142
US 5,470,661 ADiamond-like carbon films from a hydrocarbon helium plasma1995340
US 5,635,245 AProcess of making abrasion wear resistant coated substrate product1997152
US 5,838,530 AApplications of protective ceramics199864
US 5,858,477 AMethod for producing recording media having protective overcoats of highly tetrahedral amorphous carbon1999170
US 5,888,593 AIon beam process for deposition of highly wear-resistant optical coatings1999192
US 5,900,342 APhotoconductive element having an outermost layer of a fluorinated diamond-like carbon and method of making the same199974
US 6,002,208 AUniversal cold-cathode type ion source with closed-loop electron drifting and adjustable ion-emitting slit1999128
US 6,261,693 B1Highly tetrahedral amorphous carbon coating on glass2001185
US 6,280,834 B1Hydrophobic coating including DLC and/or FAS on substrate2001110
US 6,284,377 B1Hydrophobic coating including DLC on substrate2001159
US 6,303,225 B1Hydrophilic coating including DLC on substrate2001197
US 6,303,226 B2Highly tetrahedral amorphous carbon coating on glass2001131
US 6,312,808 B1Hydrophobic coating with DLC & FAS on substrate2001102
US 6,335,086 B1Hydrophobic coating including DLC on substrate2002112
US 6,338,901 B1Hydrophobic coating including DLC on substrate2002151
US 6,447,891 B1Low-E coating system including protective DLC2002164
US 6,461,731 B1Solar management coating system including protective DLC2002138
US 6,531,182 B2Method of making a coated article including DLC and FAS200363
US 2003118860 A1Hydrophilic surfaces carrying temporary protective covers—35
US 6,592,992 B2Hydrophilic coating including DLC2003108
US 6,592,993 B2Coated article with DLC inclusive layer(s) having increased hydrogen content at surface area200374

Non-Patent Literature (5)

  • "Feasibility Study of RF Sputtered ZnO Film for Surface Micromachining", Bhatt et al., Surface & Coatings Technology, 198 (2005) pp. 304-308.
  • "Hybrid AC EL Structures with Thin Protective ZnO Film", Tsvetkova et al., Journal of Physics: Conference Series 113 (2008) pp. 1-4.
  • "Low-Emissivity Coating of Amorphous Diamond-Like Carbon/Ag-Alloy Multilayer on Glass" Chiba et al., Applied Surface Science 246 (2005) pp. 48-51.
  • U.S. Appl. No. 11/699,080, filed Jan. 29, 2007.
  • U.S. Appl. No. 11/798,920, filed May 17, 2007.