Economical process of manufacturing very fine co-ground calcium carbonate material of the GCC and PCC type, obtained products and their uses
Abstract
An object of the present invention is to provide a process to obtain a calcium carbonate material comprising GCC and PCC, presenting a fraction of particles finer than 1 μm of greater than 80%, preferably of greater than 85%, more preferably of greater than 90%, and even more preferably of greater than 95%, and a specific surface area of less than 25 m 2 /g, in a cost efficient manner, wherein GCC and PCC are co-ground, possibly with at least another mineral material. An other object of the present invention lies in the co-ground calcium carbonate material in the form of an aqueous suspension and in the form of a dry product. An other object of the present invention lies in the uses of such products in any sector making use of mineral material, and notably in the paper, paint and plastic industries.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 0.
Claims (19)
- Claim 1Independent Claim
A process of manufacturing a co-ground calcium carbonate material comprising GCC and PCC, said process comprising the steps of: (a) providing GCC in an aqueous suspension, (b) co-grinding the aqueous suspension of GCC and an aqueous suspension of PCC, optionally with at least another mineral material, (c) optionally screening and/or upconcentrating the co-ground calcium carbonate material obtained following step (b), (d) optionally drying the co-ground calcium carbonate material obtained following step (b) or (c), wherein the material obtained from step (b) is characterized as having greater than 95% particles finer than 1 μm and a BET specific surface area less than 25 m 2 /g.
- Claim 2Depends on #1
The process according to claim 1 , wherein the material obtained from step (b) is characterized as having a BET specific surface area less than 20 m 2 /g.
- Claim 3Depends on #1
The process according to claim 1 , wherein the material obtained from step (b) is characterized as having BET specific surface area less than 18 m 2 /g.
- Claim 4Depends on #1
The process according to claim 1 , wherein the material obtained from step (b) is characterized as having a BET specific surface area less than 15 m 2 /g.
- Claim 5Depends on #1
The process according to claim 1 , wherein in step (a), the GCC is provided as an aqueous suspension having a solids content from 20 to 80%.
- Claim 6Depends on #1
The process according to claim 1 , wherein in step (a), the GCC is provided as an aqueous suspension having a solids content of from 50 to 75%.
- Claim 7Depends on #1
The process according to claim 1 , wherein in step (a), the GCC is provided as an aqueous suspension having a solids content of from 50 to 70%.
- Claim 8Depends on #1
The process according to claim 1 , wherein step (c) is carried out.
- Claim 9Depends on #1
The process according to claim 1 , wherein step (d) is carried out.
- Claim 10Depends on #1
The process according to claim 1 , wherein the co-grinding of GCC and PCC during step (b) is conducted in an aqueous medium at a calcium carbonate concentration of 20 to 80% by dry weight of calcium carbonate.
- Claim 11Depends on #1
The process according to claim 1 , wherein the co-grinding of GCC and PCC during step (b) is conducted in an aqueous medium at a calcium carbonate concentration of 50 to 75% by dry weight of calcium carbonate.
- Claim 12Depends on #1
The process according to claim 1 , wherein the co-grinding of GCC and PCC during step (b) is conducted in an aqueous medium at a calcium carbonate concentration of 50 to 70% by dry weight of calcium carbonate.
- Claim 13Depends on #1
The process according to claim 1 , wherein 0 to 2% by weight of at least one dispersing and/or grinding aid agent relative to total dry mineral material is added before, during or after step (b).
- Claim 14Depends on #1
The process according to claim 1 , wherein 0.2 to 1.4% by weight of at least one dispersing and/or grinding aid agent relative to total dry mineral material is added before, during or after step (b).
- Claim 15Depends on #1
The process according to claim 1 , wherein 0.5 to 1.2% by weight of at least one dispersing and/or grinding aid agent relative to total dry mineral material is added before, during or after step (b).
- Claim 16Depends on #1
The process according to claim 1 , wherein the co-grinding of GCC and PCC during step (b) is conducted in the presence of at least another mineral material selected from talc, clay, Al 2 O 3 , Ti 2 O 2 or mixtures thereof.
- Claim 17Depends on #1
The process according to claim 1 , wherein the co-grinding of GCC and PCC during step (b) is conducted in the presence of at least another mineral material selected among from talc, clay or mixtures thereof.
- Claim 18Depends on #1
The process according to claim 1 , wherein the co-grinding of GCC and PCC during step (b) is conducted in the presence of talc.
- Claim 19Depends on #1
The process according to claim 1 , wh
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATIONS This is a continuation-in-part of U.S. application Ser. No. 11/992,116, filed Jun. 23, 2008, now abandoned, which is a U.S. national phase of PCT Application No. PCT/IB2006/002649, filed Sep. 12, 2006, and claims priority to European Application No. 05077111.2, filed Sep. 16, 2005, the contents of which is incorporated by reference herein. It is an object of the present invention to provide a process to obtain a calcium carbonate material comprising GCC (ground calcium carbonate) and PCC (precipitated calcium carbonate). The material is appropriate for use in a number of domains, for example in the paper industry. It is also an object of the present invention to provide a process to obtain a calcium carbonate material comprising GCC and PCC, presenting a fraction of particles finer than 1 μm of greater than 80%, preferably of greater than 85%, more preferably of greater than 90%, and even more preferably of greater than 95%, and a BET specific surface area of less than 25 m 2 /g. When the fraction of particles finer than 1 μm is greater than 95%, the BET specific surface area is preferably less than 25 m 2 /g. When the fraction of particles finer than 1 μm is greater than 90%, greater than 85%, and greater than 80%, the BET specific surface area is preferably less than 20 m 2 /g, less than 18 m 2 /g, and less than 15 m 2 /g, respectively. Such a material leads to superior properties of paper coated with such a material, notably in terms of gloss. It is also an object of the present invention to provide a process to obtain a calcium carbonate material comprising GCC and PCC, with the above mentioned granulometric characteristics, wherein GCC and PCC are co-ground, possibly with at least another mineral material. Another object of the present invention lies in the co-ground calcium carbonate material (i.e.: aqueous mineral slurries containing the co-ground GCC and PCC and dry product
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (18)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (6)
- Faber, et al. "Horizontal Mill Friendly Ceramic Media With Improved Efficiency " Paint and Coatings Industry Magazine; Apr. 2001, pp. 30-38.
- International Search Report dated Nov. 1, 2007 for PCT Application No. PCT/IB2006/002655.
- Mühlmeier: Mahltechnik-Technische Info: Internet Citation, Jul. 2003.
- Mühlmeier: Mahltechnik—Technische Info: Internet Citation, Jul. 2003.
- Written Opinion of the International Searching Authority for PCT Application No. PCT/IB2006/002655.
- Written Opinion of the International Searching Authority for PCT Application No. PCT/IB2006/002655. Nov. 1, 2007.