Method for fabricating low-k dielectric and Cu interconnect
Abstract
A system and method for improving the performance of an integrated circuit by lowering RC delay time is provided. A preferred embodiment comprises adding a reactive etch gas to the ash/flush plasma process following a low-k dielectric etch. The illustrative embodiments implement a removal of the damage layer that is formed during a low-k dielectric etch.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of manufacturing an integrated circuit comprising: forming a low-k dielectric layer on a wafer; forming a photoresist layer over the low-k dielectric layer; etching the low-k dielectric layer; and removing the photoresist layer by performing an ash/flush plasma process on exposed portions of the low-k dielectric layer, the ash/flush plasma process using a combined ash/flush gas, wherein the combined ash/flush gas comprises an ash/flush gas with a percentage of a reactive etching gas, the ash/flush plasma process not etching the low-k dielectric layer.
- Claim 2Depends on #1
The method of claim 1 , wherein the ash/flush gas is chosen from a group consisting essentially of O 2 , CO, CO 2 , N 2 , N 2 /H 2 , NH 3 , and combinations thereof.
- Claim 3Depends on #1
The method of claim 1 , wherein the reactive etching gas is chosen from a group consisting essentially of C
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.