Low shrinkage, dyeable MPD-I yarn
Abstract
The invention relates to a continuous dry spinning process for preparing a fiber from a polymer solution having concentrations of polymer, salt, solvent and water. After the fiber is extruded and quenched, the fiber is placed in contact with a conditioning solution comprising concentrations of solvent, salt, and water. The conditioning solution acts upon the fiber to plasticize the fiber prior to being drawn. The conditioning solution has concentrations of solvent, salt, and water so that the fiber is plasticized to the extent necessary for drawing but does not plasticize the fiber to such an extent as to re-dissolve the fiber into a polymeric solution. A heat-treated fiber manufactured from this process has improved shrinkage and can be colored to darker shades.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 4.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A poly(metaphenylene isophthalamide) polymer fiber, said fiber, before coloration with a dye, shrinks linearly 0.4 percent or less when exposed to 285 degrees Centigrade for 30 minutes; and said fiber, after contact with an aqueous red dye solution for 1 hour at 120 degrees Centigrade, has an “L” value coloration of at least 40 units lower than the “L” value of the fiber before coloration; wherein the fiber is manufactured by a continuous dry spinning process the following steps, in order, comprising: extruding a solution through a shaped orifice into the fiber at a temperature of 110 degrees
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗