Method and installation for the production of steel products having an optimum surface quality

5Forward Citations (#19124080 Global)
0.3/yrCitation Velocity (#22606329 Global)
2.87Citation PageRank (#8116151 Global)
19Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Disclosed are a method and an installation for producing steel products ( 1 ) having an optimum surface quality, especially extremely low carbon contents (UCL steel or IF steel), nitrogen contents, total oxygen contents, high-strength or stainless steel qualities. According to the invention, the liquid steel is cast into a thin slab ( 5 a ) from a process route ( 10, 11, 12 , or 13 ) that is selected according to the desired final structure ( 9 ) based on an electric-arc furnace ( 2 b ), is descaled, cut into billets ( 15 ) having a partial length, optionally descaled once again, subjected to final descaling downstream from a holding furnace ( 16 ), milled in a finishing mill train ( 6 a ), rolled up in a rolling station ( 20 ) located downstream from the last finishing mill stand ( 19 ) or downstream from a cooling section ( 21 ), and the final structure ( 9 ) is adjusted in the cooling section ( 21 ) according to the desired steel quality by cooling on a run-out roller table ( 22 ), whereupon the rolling stock ( 1 a ) is completely rolled up in a second rolling station ( 23 ).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 5.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    Method for producing steel products ( 1 ) with optimum surface quality of an ultralow carbon, high-strength and/or stainless steel grade, comprising the steps of: melting ( 2 ) the steel and treating the steel in a ladle metallurgy installation ( 3 ); subsequently continuously casting the steel ( 4 ) into a thin slab ( 5 a ) in a continuous casting mold ( 14 ), partially deforming, cutting the slab into partial strand lengths ( 15 ), descaling ( 28 ), heating to rolling temperature and homogenizing in a soaking furnace ( 16 ), descaling again and rolling in a finishing mill ( 6 a ), coilin

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (19)

Non-Patent Literature (5)

  • Brascugli G et al: "First CSP Plant for Stainless Steel . . .", Stahl und Eisen, BD. 121, No. 3, Mar. 15, 2001, pp. 63-71.
  • Database WPI, Section CH, Week 198641, Derwent Publications Ltd. London GB, & JP 61194108 A (Daido Tokushuko KK), Aug. 28, 1986.
  • Kreuger B et al, "Saldanhe Steel-Die Neue Minimill . . .", Stahl und Eisen, Verlag Stahleisen GMBH, BD, 117, No. 11, Nov. 10, 1997, pp. 81-93, 154.
  • Mishra, B. ASM Handbooks Online. "Steelmaking Practices and Their Influence on Properties". downloaded on Sep. 24, 2010 from http://products.asminternational.org/hbk/index.jsp. Copyright 2002.
  • Patent Abstracts of Japan, BD. 0091, No. 7, (M-378), May 11, 1985 & JP 59229268 A (Shin Nippon Seitetsu KK), Dec. 22, 1984.