Etchant composition, patterning conductive layer and manufacturing flat panel, display device using the same
Abstract
An etchant composition that allows simplification and optimization of semiconductor manufacturing process is presented, along with a method of patterning a conductive layer using the etchant and a method of manufacturing a flat panel display using the etchant. The etchant includes nitric acid, phosphoric acid, acetic acid, and an acetate compound in addition to water.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 1.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A composition of etchant, comprising: nitric acid of about 2 weight % to about 5 weight %; phosphoric acid of about 50 weight % to about 77 weight %; acetic acid of about 1 weight % to about 25 weight %; acetate compound of about 1 weight % to about 10 weight %; and water of residual quantity.
- Claim 2Depends on #1
The composition according to claim 1 , wherein the acetate compound includes at least one anion of sodium (Na), potassium (K), ammonia (NH3), calcium (Ca), and aluminum (Al).
- Claim 3Depends on #1
The composition according to claim 1 , wherein the acetate compound is an acid salt.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2013248374 A1 | Chemical polishing of aluminum | — | 0 |