US 7,985,635 B2#129137450 Most CitedExpiredUnited States (USPTO)Utility

Laser process

0Forward Citations (#129137450 Global)
0.0/yrCitation Velocity (#129137450 Global)
0.56Citation PageRank (#129137450 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A laser annealing process for recovering crystallinity of a deposited semiconductor film such as of silicon which had undergone morphological damage, said process comprising activating the semiconductor by irradiating a pulsed laser beam operating at a wavelength of 400 nm or less and at a pulse width of 50 nsec or less onto the surface of the film, wherein, said deposited film is coated with a transparent film such as a silicon oxide film at a thickness of from 3 to 300 nm, and the laser beam incident to said coating is applied at an energy density E (mJ/cm 2 ) provided that it satisfies the relation: log 10 N ≦−0.02( E −350), where N is the number of shots of the pulsed laser beam.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a semiconductor device comprising: covering a semiconductor with a transparent film; introducing phosphorus into said semiconductor by permeating said transparent film by ion doping; and irradiating said semiconductor with a beam of laser pulses in order to activate said phosphorus in said semiconductor where the laser pulses have a wavelength of 400 nm or shorter; wherein an energy density E of each of said laser pulses in units of mJ/cm 2 and the number N of said laser pulses satisfies the relation log 10 N<−0.02(E−350) where N is not less than one and not grea

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein said semiconductor is a semiconductor film formed over a substrate.

  3. Claim 3Depends on #1

    The method according to claim 1 , wherein said energy density

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,667,832 ALight-conducting structure comprising crossed lenticular gradient index plates197249
US 4,059,461 AMethod for improving the crystallinity of semiconductor films by laser beam scanning and the products thereof1977197
US 4,151,008 AMethod involving pulsed light processing of semiconductor devices1979205
US 4,155,779 AControl techniques for annealing semiconductors197943
JP S5532026 ALiquid crystal display panel—81
US 4,198,246 APulsed laser irradiation for reducing resistivity of a doped polycrystalline silicon film198046
US 4,262,208 APhoto-electrical detecting apparatus198130
US 4,305,640 ALaser beam annealing diffuser198162
US 4,309,224 AMethod for manufacturing a semiconductor device1982141
US 4,309,225 AMethod of crystallizing amorphous material with a moving energy beam1982351
JP S5783745 AFormation of shock-proof end piece for control cable—5
US 4,370,175 AMethod of annealing implanted semiconductors by lasers1983157
US 4,379,727 AMethod of laser annealing of subsurface ion implanted regions198352
JP S58127318 AForming method for single-crystal film on insulating layer—45
JP S58191420 AForming mehtod for single crystal silicon film—10
US 4,431,459 AFabrication of MOSFETs by laser annealing through anti-reflective coating198450
US 4,436,557 AModified laser-annealing process for improving the quality of electrical P-N junctions and devices198448
JP S5945089 ABuild-up welding method—18
US 4,462,150 AMethod of forming energy beam activated conductive regions between circuit elements198439
US 4,468,855 AMethod of making aluminum gate self-aligned FET by selective beam annealing through reflective and antireflective coatings1984153
US 4,473,433 AProcess for producing dielectrically isolated single crystal silicon devices198427
US 4,475,027 AOptical beam homogenizer1984289
US 4,484,334 AOptical beam concentrator198433
JP S605508 AManufacture of semiconductor crystal thin film—4
US 4,497,015 ALight illumination device1985202
US 4,500,365 ALaser treating implanted semiconductor surface through photo-resist layer198520
US 4,536,231 APolysilicon thin films of improved electrical uniformity198525
US 4,546,009 AHigh-mobility amorphous silicon displaying non-dispersive transport properties198514
JP S60224282 AManufacture of semiconductor device—10
JP S60227484 AManufacture of photoelectric conversion semiconductor device—18

Non-Patent Literature (5)

  • "Applications of Excimer Lasers in Microelectronics", Tim McGrath, Lasertechnics, Inc., Albuquerque, New Mexico, Solid State Technology/Dec. 1983, pp. 165-169.
  • "Crystallization of Amorphous Silicon by Excimer Laser Annealing with a Line Shape Beam Having A Gaussian Profile", Young Min Jhon et al., Jpn. J. Appl. Phys. vol. 33 (1994), pp. L1438-1441.
  • "Enlargement of Poly-Si Film Grain Size by Excimer Laser Annealing and its Application to High-Performance Poly-Si Thin Film Transistor", Hiroyuki Kuriyama et al., Jpn. J. App. Phys., vol. 30, No. 12B, Dec. 1991, pp. 3700-3703.
  • "Formation of p-n Junctions and Silicides in Silicon Using a High Performance Laser Beam Homogenization System", M. Wagner et al., Applied Surface Science 43 (1989), pp. 260-263.
  • "Improving the Uniformity of Poly-Si Films Using a New Excimer Laser Annealing Method for Giant-Microelectronics", Hiroyuki Kuriyama et al., Jpn. J. Appl. Phys. vol. 31, Part 1, No. 12B, Dec. 1992, pp. 4550-4554.