Method for quenching steel
Abstract
A polymeric quenchant. The polymeric quenchant comprises an inorganic nanoparticle, a water-soluble polymer, and water, wherein a weight ratio of the inorganic nanoparticle, water-soluble polymer and water is about 0.05-5:1-5:100. The cooling rate of steel during a quenching process can be adjusted by regulating the components and ratios of the adjusted by regulating the components and ratios of the polymeric quenchant to achieve desirable steel properties.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 0.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for quenching steel, comprising: providing a steel; heating the steel; and quenching the steel using the polymeric quenchant, wherein the steel has a temperature of maximum cooling rate exceeding 500° C., and a cooling rate at 300° C. less than 30° C./sec during the quenching, wherein the polymeric quenchant comprises an inorganic nanoparticle, a water-soluble polymer, and water, wherein a weight ratio of the inorganic nanoparticle, water-soluble polymer and water is about 0.05-5:1-5:100, and the inorganic nanoparticle is talc, smectite clay, vermiculite, halloysite, sericite, saponit
- Claim 2Depends on #1
The method as claimed in claim 1 , wherein the steel has a maximum cooling rate of about 60-160° C./sec, a temperature of maximum cooling rate exceeding 500° C., and a cooling rat
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗