Patents
US 7,980,098 B2#145618848 Most CitedActiveUnited States (USPTO)Utility

Method for producing an optical component of synthetic quartz glass with enhanced radiation resistance, and blank for producing the component

0Forward Citations (#145618848 Global)
0.0/yrCitation Velocity (#145618848 Global)
0.56Citation PageRank (#145618848 Global)
13Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

To optimize an optical component of synthetic quartz glass, in the case of which a quartz glass blank is subjected to a multistage annealing treatment, with respect to compaction and central birefringence, the present invention suggests a method comprising the following steps: (a) a first treatment phase during which the quartz glass blank is treated in an upper temperature range between 1130° C. and 1240° C., (b) cooling the quartz glass blank at a first-higher-mean cooling rate to a quenching temperature below 1100° C., a fictive temperature with a high mean value of 1100° C. or more being reached in the quartz glass, (c) a second treatment phase which comprises cooling of the quartz glass blank at a second-lower-mean cooling rate, and in which the quartz glass blank is treated in a lower temperature range between 950° C. and 1100° C. such that a fictive temperature is reached in the quartz glass with a low mean value which is at least 50° C. lower than the high mean value of the fictive temperature according to method step (b).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing an optical component of synthetic quartz glass with radiation resistance in a microlithographic device at an operating wavelength below 250 nm, said method comprising: providing a quartz glass blank with a hydroxyl group content of less than 250 wtppm and subjecting the quartz glass blank to a multi-stage annealing treatment comprising the following steps: (a) a first treatment phase during which the quartz glass blank is treated in an upper temperature range between 1130° C. and 1240° C. during a first treatment period; (b) cooling the quartz glass blank at a first mean

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (1)

  • EPODOC English language abstract for JP2002121038, Apr. 23, 2002.