Abstract

In manufacturing a device using an organic TFT, it is essential to develop an element in which a channel length is short or a channel width is narrow to downsize a device. Based on the above, it is an object of the present invention to provide an organic TFT in which characteristic is improved. In view of the foregoing problem, one feature of the present invention is that an element is baked after an organic semiconductor film is deposited. More specifically, one feature of the present invention is that the organic semiconductor film is heated under atmospheric pressure or under reduced pressure. Moreover, a baking process may be carried out in an inert gas atmosphere.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 33 · Forward citations: 1.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing an organic semiconductor element, comprising the steps of: forming a gate electrode; forming an organic semiconductor film over the gate electrode; forming a source electrode and a drain electrode over the organic semiconductor film; and heating the organic semiconductor film under atmospheric pressure or under reduced pressure in an inert gas atmosphere after completion of the formation of the organic semiconductor film.

  2. Claim 2Independent Claim

    A method for manufacturing an organic semiconductor element, comprising the steps of: forming a gate electrode; forming an organic semiconductor film over the gate electrode; forming a source electrode and a drain electrode over the organic semiconductor film; and heating the organic semiconductor film under atmospheric pressure or under reduced pressure after completion of the formation of the organic

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (33)

PatentTitleYearCitations
EP 0,716,458 A2Method of making an organic thin film transistor, and article made by the method—22
JP H08228035 AThin film transistor device and manufacture thereof—33
US 5,574,291 AArticle comprising a thin film transistor with low conductivity organic layer1996152
JP H09116163 AField effect transistor, and its manufacture—16
US 5,705,826 AField-effect transistor having a semiconductor layer made of an organic compound1998213
US 5,946,551 AFabrication of thin film effect transistor comprising an organic semiconductor and chemical solution deposited metal oxide gate dielectric1999248
US 6,150,668 AThin-film transistor monolithically integrated with an organic light-emitting diode2000285
US 6,207,472 B1Low temperature thin film transistor fabrication2001139
US 6,300,988 B1Liquid crystal display apparatus having patterned insulating layer formed over a substrate except for a region on the gate electrode2001132
US 6,326,640 B1Organic thin film transistor with enhanced carrier mobility2001163
US 6,335,539 B1Method for improving performance of organic semiconductors in bottom electrode structure2002183
US 2002012080 A1Liquid crystal display apparatus—47
US 2002022299 A1Aqueous-based photolithography on organic materials—45
US 6,429,457 B1Field-effect transistor200244
US 6,433,359 B1Surface modifying layers for organic thin film transistors2002260
US 6,452,207 B1Organic semiconductor devices200297
US 2002155729 A1Semiconductor device encapsulation—88
US 2002164835 A1Organic n-channel semiconductor device of N,N' 3,4,9,10 perylene tetracarboxylic diimide—81
US 2002179901 A1Organic semiconductor device and process of manufacturing the same—72
WO 03,016,599 A1Organic semiconductor element—110
US 6,528,816 B1Integrated inorganic/organic complementary thin-film transistor circuit and a method for its production200398
US 6,635,508 B2Organic semiconductor device and process of manufacturing the same200364
US 2003211649 A1Organic thin-film transistor, organic thin-film transistor sheet and manufacturing method thereof—60
JP 2003338629 AOrganic thin-film transistor—15
EP 1,416,069 A1Organic semiconductor element—27
US 2004191952 A1Method of manufacturing high-mobility organic thin films using organic vapor phase deposition—25
US 6,905,908 B2Method of fabricating organic field effect transistors200517
US 2005176196 A1Method of fabricating organic field effect transistors—11
US 7,015,502 B2Organic semiconductor device and process of manufacturing the same200629

Non-Patent Literature (4)

  • Lee.J et al., "Annealing Effects on the Electrical Characteristics of Pentacene Thin Film Transistors,",Journal of the Korean Physical Society, Mar. 1, 2001, vol. 38, No. 3, pp. 282-285.
  • Notice on First Office Action dated Nov. 28, 2008 in Chinese Patent Application No. 200410011448.X, People's Republic of China, 7 pages; with English translation, 12 pp.
  • Yagi I. et al; "Pentacene FET Fabricated On Surface Treated SiO2/Si Substrate," 50th Japan Society of Applied Physics and Related Societies, Extended Abstract (Mar. 2003 in Kanagawa University); 29a-Lambda-9, Mar. 2005; p. 1418.
  • Yagi I. et al; "Pentacene FET Fabricated On Surface Treated SiO2/Si Substrate," 50th Japan Society of Applied Physics and Related Societies, Extended Abstract (Mar. 2003 in Kanagawa University); 29a-Λ-9, Mar. 2005; p. 1418.