Temperature-regulating fiber and a method of making the same
Abstract
A temperature-regulating fiber may include a spun phase change polymeric material that may include a plurality of phase change polymer blocks. The fiber may have a fixity ratio of at least 80% and a recovery ratio of at least 74%.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 7.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A temperature-regulating fiber, comprising: a spun phase change polymeric material comprising a plurality of phase change polymer blocks, wherein said fiber comprises a fixity ratio of at least 80% and a recovery ratio of at least 74%.
- Claim 2Depends on #1
The fiber of claim 1 , wherein said phase change polymer blocks are blocks of a polymer selected from the group consisting of polyethylene glycol, polytetramethylene glycol, poly(ethylene adipate) glycol, poly(ε-caprolactone) glycol, poly(tetrahydrofuran) glycol, poly(butylene adipate) glycol, polypropylene glycol, polypropylene malonate, polyneopentyl glycol sebacate, polypentane glutarate, polyvinyl myristate, polyvinyl stearate, polyvinyl laurate, polyhexadecyl methacrylate, polyoctadecyl methacrylate, and mixtures thereof.
- Claim 3Depends on #1
The fiber of claim 1 , wherein said spun phase change polymeric material co