Patents
US 7,964,456 B2#113435394 Most CitedExpiredUnited States (USPTO)Utility

Method of fabricating polysilicon thin film and thin film transistor using polysilicon fabricated by the same method

0Forward Citations (#113435394 Global)
0.0/yrCitation Velocity (#113435394 Global)
0.56Citation PageRank (#113435394 Global)
9Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of fabricating a polysilicon thin film produces a polysilicon thin film which is used to make a thin film transistor. The method includes depositing a silicon film containing amorphous silicon on a substrate, and performing thermal treatment on the silicon film at a predetermined temperature in an H 2 O atmosphere. Accordingly, the crystallization temperature and thermal treatment time are decreased when the amorphous silicon is crystallized by a solid phase crystallization method, and this prevents the substrate from being bent due to application of a thermal treatment process for a long time and at a high temperature. As a result of the invention, a polysilicon thin film having superior crystallization properties is obtained. Use of the polysilicon thin film in a thin film transistor results in the reduction of defects in the thin film resistor.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating a polysilicon thin film, comprising: depositing a silicon film containing amorphous silicon on a substrate; and crystallizing the silicon film via solid phase crystallization by performing thermal treatment on the silicon film in an atmosphere that includes H 2 O at a predetermined temperature; wherein a pressure of the H 2 O is at least 10,000 Pa and the thermal treatment has a duration of 10 minutes or less.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the predetermined temperature is in a range of 550° C. to 750° C.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein the predetermined temperature is in a range of 600° C. to 700° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (4)

  • "Polycrystalline Silicone Thin-film Transistor Fabricated by Defect Reduction Methods", to Watakabe, et al. IEEE Transaction on Electron Devices, vol. 49, No. 12, Dec. 2002.
  • Korean Office Action of the Korean Patent Application No. 2004-11146, issued on Feb. 22, 2006.
  • Office action from the Japanese Patent Office issued in Applicant's corresponding Japanese Patent Application No. 2004-340254 dated Mar. 24, 2009.
  • Watakabe et al "Polycrysatlline Silicon Thin-Film Transistors Fabricated by Defect reduction Mehods" IEEE Transactions on Electronic Devices, vol. 49, No. 12Dec. 2002.