Method for producing nanocrystalline magnet cores, and device for carrying out said method
Abstract
The invention relates to a method and to a device for carrying out a manufacturing process in which all magnet cores to be produced are first continuously crystallized. Depending on whether the required hysteresis loops should be round, flat or rectangular, the magnet cores are either immediately finished, that is enclosed in housings, conditioned to a rectangular hysteresis loop in a direct-axis magnetic field or to a flat hysteresis loop in a magnetic cross-field and then finished.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 3.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for the production of magnet cores comprising an iron-based soft magnetic alloy wherein at least 50% of the alloy structure is occupied by fine-crystalline particles with an average particle size of 100 nm or less, comprising: a) preparing an alloy melt; b) producing an amorphous alloy strip from the alloy melt by means of quick-hardening technology; c) winding of the amorphous strip to form unstacked amorphous magnet cores; d) heat treating of the unstacked amorphous magnet cores to form nanocrystalline magnet cores, comprising conveying each unstacked amorphous magnet core through
- Claim 2Independent Claim
The process according to claim