Patents
US 7,964,014 B2#142688181 Most CitedActiveUnited States (USPTO)Utility

Metal oxide-bearing green pellets for reducing furnace, method of production of same, method of reduction of same, and reduction facility

0Forward Citations (#142688181 Global)
0.0/yrCitation Velocity (#142688181 Global)
0.56Citation PageRank (#142688181 Global)
35Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a method and facility for preventing crumbling and powderization of green pellets when producing high strength green pellets using a powder feedstock and using the pellets in a rotary hearth reducing furnace and for efficiently reducing the same. It comprises kneading by a kneader 5 a feedstock of a powder of a fine particle size (20 to 80 wt % having size of not more than 10 μm) including a metal oxide and carbon-bearing powder fed from a feed storage tank 1 and producing green pellets by a pan type pelletizer 7 . The green pellets are screened by a pellet screen 9 , then dried by a pellet dryer 11 and reduced by firing in a rotary hearth reducing furnace 13 . At that time, the green pellets are continuously conveyed to prevent crumbling.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 35 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of reduction of metal oxide-bearing green pellets for a reducing furnace characterized by charging (i) iron oxide-bearing green pellets for a reducing furnace obtained by shaping a feed powder containing a metal oxide-bearing powder and 5 to 30 wt % of a carbon-bearing powder, wherein, when shaping the green pellets, three or more types of feed powder, including at least two types of iron containing feed powder, are placed in separate storage bins, a mixing ratio of a mixture of feed powders is determined so that the mixture of said feed powder includes 20 to 80 wt % of powder particl

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (35)

PatentTitleYearCitations
US 3,374,085 AProcess for producing aggregate containing oxygen steel process dust196822
AU 432,037 B2Agglomeration of oxygen furnace dust19734
US 3,765,869 AMethod of producing iron-ore pellets197321
US 3,969,103 AMethod of producing ball agglomerated particulate material197617
FR 2,343,054 A1Roasted iron ore pellets with controlled macroporosity - which raises softening point and improves degree of redn. obtd.—3
US 4,093,448 AMethod of producing pellets from ore concentrates197817
JP S5466314 AManufacture of reduced pellets—8
US 4,231,797 AFired iron-ore pellets having macro pores198022
US 4,257,806 AFired iron-ore pellets having macro pores and process for producing the same198126
CA 1,099,518 AFired iron-ore pellets having macro pores and process for producing the same19812
JP S61207526 AManufacture of raw material for iron manufacture excelling in reducing property—9
JP S62220590 AProduction of granular fuel—8
US 4,701,214 AMethod of producing iron using rotary hearth and apparatus1987158
JP S62270730 AMethod for molding green pellet of iron ore—2
US 4,840,774 AProcess for the production of zirconium tetrachloride from dissociated zircon198910
JP H01247534 ATreatment of ore as stock for smelting and reducing—4
JP H04165025 AManufacture of reduced pellet—6
US 5,186,741 ADirect reduction process in a rotary hearth furnace199390
CN 1,110,325 AAlkaline carbonaceous flue dust powder cooled agglomerated pellet—4
JP H07278687 AProduction of cold bonded briquette—6
US 5,601,631 AProcess for treating metal oxide fines199764
JP H09279258 AMethod for agglomerating iron-making dust—6
US 5,730,775 AMethod for rapid reduction of iron oxide in a rotary hearth furnace199891
US 5,738,694 AProcess for recovering iron from iron-containing material199817
JP H10147806 AProduction of high quality reduced iron from ironmaking dust—11
JP H10192894 AMethod for treating sludge containing oil and iron—12
US 5,865,875 AProcess for treating metal oxide fines199941
EP 0,916,742 A1Method of producing iron oxide pellets with low bentonite content—38
EP 0,924,304 A1Method of producing reduced iron pellets—15
JP H11193423 AIron oxide pellet and its manufacture, and reduced iron pellet and its manufacture—22

Non-Patent Literature (3)

  • Ajersch, "Chemical and Physical Characteristics Affecting the Reduction Kinetics of Iron Oxide Pellets with Solid Carbon", Canadian Metallurgical Quarterly 26:137-144 (1987).
  • Sintering and Pelletizing, vol. 20, No. 5, pp. 7-12, Sep. 1995.
  • Xia et al. "Recent Research on the Pyrometallurgical and Hydrometallurgical Treatment of Electric Arc Furnace Flue Dust" Intertech 10th International Converence on Steel Mill Wastes by Products, 1997, pp. 138-196.