Texturing semiconductor substrates
Abstract
Semiconductors are textured with aqueous solutions containing non-volatile alkoxylated glycols, their ethers and ether acetate derivatives having molecular weights of 170 or greater and flash points of 75° C. or greater. The textured semiconductors can be used in the manufacture of photovoltaic devices.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 4.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method comprising: a) providing a semiconductor substrate; and b) applying an aqueous solution comprising one or more compounds chosen from alkoxylated glycols, their mono-methyl ether and mono-methyl ether acetate derivatives comprising a molecular weight of 170 g/mole or greater and a flash point of 75° C. or greater, and one or more alkaline compounds to the semiconductor substrate to texture the semiconductor substrate.
- Claim 2Depends on #1
The method of claim 1 , wherein the one or more compounds chosen from alkoxylated glycols, their mono-methyl ether and mono-methyl ether acetate derivatives have a formula: RO(C x H 2x O) m Y (I) wherein R is —CH 3 or —H, Y is —H or —C(O)CH 3 , and m is an integer of 3 or greater and x is an integer of 3 to 6.
- Claim 3Depends on #1
The method of claim 1 , wherein the alkoxylated glycols have a formula: HO(CH 2 CH
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗