Enhanced alumina layer with texture
Abstract
A refined method to produce textured α-Al 2 O 3 layers in a temperature range of 750-1000° C. with a controlled texture and substantially enhanced wear resistance and toughness than the prior art is disclosed. The α-Al 2 O 3 layer is formed on a bonding layer of (Ti,Al)(C,O,N) with increasing aluminum content towards the outer surface. Nucleation of α-Al 2 O 3 is obtained through a nucleation step composed of short pulses and purges of Ti-containing and oxidizing steps. The α-Al 2 O 3 layer has a thickness ranging from 1 to 20 μm and is composed of columnar grains. The length/width ratio of the alumina grains is from 2 to 15, preferably 6 to 10. The layer is characterized by a strong (110) growth texture, measured using XRD, and by the low intensity of (012), (104), (113), (024) and (116) diffraction peaks.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of coating a substrate with an Al 2 O 3 layer wherein the α-Al 2 O 3 layer is composed of columnar α-Al 2 O 3 grains with a texture coefficient TC (110) greater than about 2.0 comprising depositing a (Ti,Al)(C,O,N) bonding layer on said substrate to provide a nucleation surface for said Al 2 O 3 , subjecting said nucleation surface to a modification treatment of a pulse treatment with a mixture of TiCl 4 and H 2 , a purge with a neutral gas and an oxidizing pulse of a gas mixture including N 2 and CO 2 in a ratio of N 2 :CO 2 from about 100 to about 200, repeating the modificat
- Claim 2Depends on #1
The method of claim 1 wherein each said pulse treatment is conducted for a time of from about 0.5 to about 5 minutes.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- Communication pursuant to Rule 82(2) EPC dated Nov. 9, 2010 issued in EP 05 445 083.8.
- Kim et al., "Effect of Partial Pressure of the Reactant Gas on the Chemical Vapour Deposition of Al2O3," Thin Solid Films, vol. 97, 1982, pp. 97-106.
- Provision of the minutes in accordance with Rule 124(4) EPC dated Jul. 19, 2010 issued in EP 05 445 083.8.
- Y. Yoursdshahyan, C. Ruberto, M. Halvarsson, V. Langer, S. Ruppi, U. Rolander and B.I. Lundqvist, Theoretical Structure Determination of a Complex Material: kappa-A1203, J. Am. Ceram. Soc. 82(6) (1999) 1365-1380).
- Y. Yoursdshahyan, C. Ruberto, M. Halvarsson, V. Langer, S. Ruppi, U. Rolander and B.I. Lundqvist, Theoretical Structure Determination of a Complex Material: κ-A1203, J. Am. Ceram. Soc. 82(6) (1999) 1365-1380).