Abstract
It is an object to provide an inexpensive alloy for heat dissipation having a small thermal expansion coefficient as known composite materials, a large thermal conductivity as pure copper, and excellent machinability and a method for manufacturing the alloy. In particular, since various shapes are required of the alloy for heat dissipation, a manufacturing method by using a powder metallurgy method capable of supplying alloys for heat dissipation, the manufacturing costs of which are low and which take on various shapes, is provided besides the known melting method. The alloy according to the present invention is a Cu—Cr alloy, which is composed of 0.3 percent by mass or more, and 80 percent by mass or less of Cr and the remainder of Cu and incidental impurities and which has a structure in which particulate Cr phases having a major axis of 100 nm or less and an aspect ratio of less than 10 are precipitated at a density of 20 particles/μm 2 in a Cu matrix except Cr phases of more than 100 nm.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 3.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A Cu—Cr alloy comprising more than 3 percent by mass and 40 percent by mass or less of Cr and the remainder of Cu and incidental impurities and comprising a structure in which particulate Cr phases having a major axis of 100 nm or less and an aspect ratio of less than 10 are precipitated at a density of 20 particles/μm 2 or more in a Cu matrix except Cr phases of more than 100 nm.
- Claim 2Depends on #1
The Cu—Cr alloy according to claim 1 , wherein the alloy has been worked into a predetermined shape by a melting method or a powder metallurgy method, subjected to infiltration and/or a solution heat treatment, cooled at a cooling rate of 30° C./min or less, and subjected to aging at a range of 500° C. or higher, and 750° C. or lower.
- Claim 3Depends on #1
The Cu—Cr alloy according to claim 1 , wherein the alloy has been molded into a predetermined shape by a powder metallurgy meth
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (19)
Non-Patent Literature (1)
- J.R. Davis, "ASM Handbook: Copper and Copper Alloys", ASM Specialty Handbook: Copper and Copper Alloys, ASM International, pp. 159-161 (2001).