Patents
US 7,951,730 B2#27294119 Most CitedActiveUnited States (USPTO)Utility

Decreasing the etch rate of silicon nitride by carbon addition

4Forward Citations (#27294119 Global)
0.3/yrCitation Velocity (#27808204 Global)
1.05Citation PageRank (#38984272 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Methods for forming silicon nitride hard masks are provided. The silicon nitride hard masks include carbon-doped silicon nitride layers and undoped silicon nitride layers. Carbon-doped silicon nitride layers that are deposited from a mixture comprising a carbon source compound, a silicon source compound, and a nitrogen source in the presence of RF power are provided. Also provided are methods of UV post-treating silicon nitride layers to provide silicon nitride hard masks. The carbon-doped silicon nitride layers and UV post-treated silicon nitride layers have desirable wet etch rates and dry etch rates for hard mask layers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a carbon-doped silicon nitride hard mask, comprising: introducing trimethylsilane into a chamber at a first flow rate; introducing silane into the chamber at a second flow rate, wherein the ratio of the second flow rate to the first flow rate is between about 50:1 and about 1:1; introducing NH 3 into the chamber; and reacting the trimethylsilane, silane, and NH 3 in the presence of RF power to deposit the carbon-doped silicon nitride hard mask on a substrate in the chamber.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the first flow rate is between about 2 sccm and about 2000 sccm, the second flow rate is between about 20 sccm and about 2000 sccm, and the NH 3 is introduced into the chamber at a flow rate of between about 100 sccm and about 15000 sccm.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the RF power is provided at a power

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,091,169 ASilicon oxide/silicon nitride mask with improved integrity for semiconductor fabrication197832
US 4,894,352 ADeposition of silicon-containing films using organosilicon compounds and nitrogen trifluoride1990308
US 5,300,322 AMolybdenum enhanced low-temperature deposition of crystalline silicon nitride199437
US 5,374,570 AMethod of manufacturing active matrix display device using insulation layer formed by the ale method1994213
US 5,503,875 AFilm forming method wherein a partial pressure of a reaction byproduct in a processing container is reduced temporarily1996216
US 5,772,773 ACo-axial motorized wafer lift199867
US 5,916,365 ASequential chemical vapor deposition1999819
US 6,079,356 AReactor optimized for chemical vapor deposition of titanium2000196
US 6,090,442 AMethod of growing films on substrates at room temperatures using catalyzed binary reaction sequence chemistry2000140
US 6,103,014 AChemical vapor deposition chamber200036
US 6,153,261 ADielectric film deposition employing a bistertiarybutylaminesilane precursor200060
US 6,200,893 B1Radical-assisted sequential CVD2001685
US 6,207,487 B1Method for forming dielectric film of capacitor having different thicknesses partly2001300
JP 2001111000 ASemiconductor element and manufacturing method thereof—104
US 6,245,192 B1Gas distribution apparatus for semiconductor processing2001324
US 6,271,054 B1Method for reducing dark current effects in a charge couple device200137
US 6,270,572 B1Method for manufacturing thin film using atomic layer deposition2001439
US 6,277,200 B2Dielectric film deposition employing a bistertiarybutylaminesilane precursor200128
US 6,284,646 B1Methods of forming smooth conductive layers for integrated circuit devices2001179
US 6,287,965 B1Method of forming metal layer using atomic layer deposition and semiconductor device having the metal layer as barrier metal layer or upper or lower electrode of capacitor2001432
EP 0,835,950 B1Reactant gas ejector head20013
US 2001030369 A1Methods and apparatus for forming a film on s substrate—28
US 6,305,314 B1Apparatus and concept for minimizing parasitic chemical vapor deposition during atomic layer deposition2001220
US 6,326,658 B1Semiconductor device including an interface layer containing chlorine200152
US 6,333,547 B1Semiconductor device and method of manufacturing the same200188
US 6,342,277 B1Sequential chemical vapor deposition2002435

Non-Patent Literature (5)

  • English translation of First Office Action dated Nov. 7, 2008, Chinese Patent Application No. 200710126049.1.
  • English translation of Notice of Registration and Grant dated Jun. 5, 2009, Chinese Patent Application No. 200710126049.1.
  • George, et al "Surface Chemistry for Atomic Layer Growth", J.Phys. Chem. 1996, vol. 100, No. 31, pp. 13121-13131.
  • International Search Report and Written Opinion of the International Searching Authority dated Apr. 11, 2005 for International Application No. PCT/US2004/027584.
  • Lee, et al. "Cyclic technique for the enhancement of highly oriented diamond film growth", Thin Solid Films 303 (1997) pp. 264-268.