Patents
US 7,947,204 B2#34016848 Most CitedExpiredUnited States (USPTO)Utility

Poly(arylene ether) compression molding

3Forward Citations (#34016848 Global)
0.2/yrCitation Velocity (#33327395 Global)
0.96Citation PageRank (#44180644 Global)
26Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for compression molding of poly(arylene ether) powder comprises introducing a powder comprising unheated poly(arylene ether) powder to compaction equipment comprising a compression mold and subjecting the powder in the compression mold to a pressure sufficient to produce an article having a density greater than the unheated poly(arylene ether) powder wherein the pressure is applied at a temperature less than the glass transition temperature of the poly(arylene ether) powder.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for compression molding of poly(arylene ether) powder, comprising: introducing a powder comprising unheated poly(arylene ether) powder to compaction equipment comprising a compression mold; and subjecting the powder in the compression mold to a pressure of 1 to 50 tons per square centimeter to produce an article having a density of about 0.6 to about 1.2 grams per cubic centimeter, a compressive strength of greater than or equal to about 25 kg, and a diameter to height ratio of 1.6 to 2.1, wherein said pressure is applied at a temperature of 0 to 65° C.

  2. Claim 2Depends on #1

    The method of claim 1 wherein the temperature is 0 to about 60° C. and the pressure is applied for about 0.1 to about 100 seconds.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein the article has a compressive strength of about 25 to about 3000 kilograms.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (26)

PatentTitleYearCitations
US 3,078,254 AHigh molecular polymers and method for their preparation1963151
US 3,265,765 ABlock polymers of monovinyl aromatic hydrocarbons and conjugated dienes1966422
US 3,297,793 AContinuous process for producing block copolymers of dienes and vinyl aromatic compounds196779
US 3,356,761 AMelt processable polyphenylene ether and process196773
US 3,402,159 AProcess for polymerizing butadiene and styrene terminated in short blocks of polystyrene196882
US 3,408,437 AMolding thermoplastic printing plates196812
US 3,594,452 APolymers prepared from monolithiumterminated block copolymers and certain diesters1971150
CA 1,264,741 ATetrahydronaphthalene derivatives as dopamine agonists19900
US 4,154,775 AFlame retardant composition of polyphenylene ether, styrene resin and cyclic phosphate1979217
GB 2,043,083 AFlame retardant polyphenylene ether compositions—108
US 4,492,805 APolyarylene ethers containing phosphorus198517
US 4,888,397 AFunctionalized polyphenylene ether from polyphenylene ether chain terminated with phenoxy moiety containing amino and hydroxy group198967
US 5,147,722 AProcess for the production of materials and materials produced by the process1992202
DE 4,140,499 A1Composites contg. polyarylene ether-ketone and/or polyphenylene sulphide and/or thermoplastic polyester - formed by press-moulding the components together at a temp. between the Tg and the m.pt. of the polymer—20
US 5,294,667 APreparation of thermoplastic molding materials based on pulverulent polyphenylene ethers and aromatic vinyl polymers19948
EP 0,640,640 A1Polyarylether agglomerates—5
US 5,767,426 AFerromagnetic powder compositions formulated with thermoplastic materials and fluoric resins and compacted articles made from the same199827
JP 2000167827 AManufacture of polyphenylene ether tablet—12
JP 2000302877 APreparation of polyphenylene ether powder with improved grain size distribution—8
US 6,194,518 B1Solid polymer dispersions and method for their preparation200111
US 6,359,043 B1Mica as flame retardant in glass filled noryl200210
WO 02,094,529 A1Tablet, process for producing the same, and molded article obtained therefrom—4
US 2002198123 A1Composition and method for foaming resin—15
US 6,534,564 B2Method of making metal-based compacted components and metal-based powder compositions suitable for cold compaction200310
EP 1,389,514 A1TABLET, PROCESS FOR PRODUCING THE SAME, AND MOLDED ARTICLE OBTAINED THEREFROM—3
US 2005098916 A1Tablet, process for producing the same, and molded article obtained therefrom—16

Non-Patent Literature (4)

  • Harper, Charles A., Modern Plastics Handbook, McGraw-Hill, Nov. 20, 2002, section 6.2.3.
  • International Search Report for International Application No. PCT/US2005/011754, mailed Aug. 24, 2005.
  • Japanese Patent No. JP51025394, Abstract only.
  • JP2003183385. Publication Date. Jul. 3, 2003. Method of Manufacturing Functional Polyphenylene Ether Having Low Molecular Weight.