Process for producing a corrosion-resistant austenitic alloy component
Abstract
An austenitic, substantially ferrite-free steel alloy and a process for producing components therefrom. This Abstract is not intended to define the invention disclosed in the specification, nor intended to limit the scope of the invention in any way.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 3.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for producing an austenitic, substantially ferrite-free component, wherein the component has a fatigue strength under reversed stresses at room temperature of greater than about 400 MPa at 10 7 load alternation, and the process comprises: (a) providing a cast piece of an alloy which comprises, in % by weight, from about 0% to about 0.35% of carbon from about 0% to about 0.75% of silicon from more than about 20.0% to about 30.0% of manganese from more than about 17.0% to about 24.0% of chromium from more than 1.90% to about 5.5% of molybdenum from about 0% to about 2.0% of tungsten f
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (25)
Non-Patent Literature (5)
- "Property Changes due to cold working", Structure and Properties of Engineering Materials, Brick et al.,1977.
- ASTM Designation: G36-94 (Reapproved 2000) "Standard Practice for Evaluating Stress-Corrosion-Cracking Resistance of Metals and Alloys in a Boiling Magnesium Chloride Solution", American Society for Testing and Materials, West Consohocken, PA, 2000, pp. 134-139.
- English Language Abstract of AT 387709, Mar. 10, 1989.
- English Language Abstract of DE 196 07 828, Oct. 17, 1996.
- English Language Abstract of DE 19758613, Oct. 29, 1998.