Patents
US 7,943,679 B2#12000777 Most CitedActiveUnited States (USPTO)Utility

Method of molding rigid polyurethane foams with enhanced thermal conductivity

9Forward Citations (#12000777 Global)
0.6/yrCitation Velocity (#13081689 Global)
1.78Citation PageRank (#17473059 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention is to a molded rigid polyurethane foam for application in appliance, having a reduced thermal conductivity at densities between 33 and 38 kg/m 3 and a process for the production of such foams. The molded rigid polyurethane foam have a ratio of applied foam density (kg/m3) to lambda (mW/mK), measured at 10° C., 24 hours after foam production from 1.65 and to 2.15 and are obtained by the process of injecting into a closed mold cavity under reduced pressure a reaction mixture at a packing factor of 1.1 to 1.9 and the reaction mixture comprises: A) an organic polyisocyanate; B) a physical blowing agent, C) a polyol composition containing at least one polyol with a functionality of 3 or greater and a hydroxyl number between 200 and 800 and a water content of 0 to 2.5 weight percent of the total polyol composition; D) catalyst and E) auxiliary substances and/or additives.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a rigid polyurethane foam having a molded density of 33 to 38 kg/m 3 and Lambda (10° C.) of less than 21 mW/m.K and a ratio of molded foam density (kg/m 3 ) to Lambda (10° C.) (mW/m.K), measured 24 hours after foam production, from 1.65 to 2.15, obtained by injecting into a closed mold cavity a reaction mixture at a packing factor of 1.03 to 1.9 wherein the mold cavity has a reduced pressure of 300 to 950 mbar and the reaction mixture comprises: A) an organic polyisocyanate; B) a physical blowing agent present in an amount from 10 to 30 weight percent of the polyol c

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗