Abstract

Silicon oxide film having, as a sublayer, a silicon nitride film layer serving as a protective film layer for 5 gate formed on silicon substrate is etched by introducing a processing gas including a gaseous mixture containing at least C 4 F 6 , Ar, O 2 and N 2 into an airtight processing chamber and carrying out a plasma treatment in a self-alignment contact process, thereby forming contact hole. For the 10 processing gas, e.g., the ratio of N 2 gas flow rate to C 4 F 6 gas flow rate ranges from 25/8 to 85/8, the ratio of O 2 and N 2 gas flow rate to C 4 F 6 gas flow rate ranges from 15/4 to 45/4 and the ratio of N 2 gas flow rate to O 2 gas flow rate ranges from 5 to 17. Accordingly, stable contact holes of 15 high aspect ratio exhibiting desirable control characteristics is formed while minimizing etching the silicon nitride film, a protective film layer for gate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An etching method comprising: feeding a processing gas into an airtight processing chamber to generate therein a plasma of the processing gas; and selectively etching a silicon oxide film against a silicon nitride film, the silicon oxide film being formed on an object to be processed disposed in the processing chamber, wherein the processing gas is a gaseous mixture including a C 4 F 6 gas, an oxygen gas, a nitrogen gas and an inert gas, and wherein an etching selectivity of the silicon oxide film to the silicon nitride film is controlled by adjusting a ratio of a total flow rate of the oxyge

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (17)

PatentTitleYearCitations
US 5,948,701 ASelf-aligned contact (SAC) etching using polymer-building chemistry199932
WO 9,957,757 A1Method for etching silicon dioxide using fluorocarbon gas chemistry—4
US 6,040,223 AMethod for making improved polysilicon FET gate electrodes having composite sidewall spacers using a trapezoidal-shaped insulating layer for more reliable integrated circuits200041
US 6,117,786 AMethod for etching silicon dioxide using fluorocarbon gas chemistry200061
WO 0,059,021 A1Enhancement of silicon oxide etch rate and substrate selectivity with xenon addition—9
JP 2001068462 APlasma etching method using selective polymer deposition md method of forming contact holes using the same—52
US 6,217,786 B1Mechanism for bow reduction and critical dimension control in etching silicon dioxide using hydrogen-containing additive gases in fluorocarbon gas chemistry200134
US 2002001963 A1Fabrication method of semiconductor integrated circuit device—34
US 2002055263 A1Oxide film etching method—5
US 2002142610 A1Plasma etching of dielectric layer with selectivity to stop layer—57
US 2003024902 A1Method of plasma etching low-k dielectric materials—64
US 6,544,429 B1Enhancement of silicon oxide etch rate and substrate selectivity with xenon addition200315
US 6,602,434 B1Process for etching oxide using hexafluorobutadiene or related fluorocarbons and manifesting a wide process window200349
US 6,617,253 B1Plasma etching method using polymer deposition and method of forming contact hole using the plasma etching method2003116
US 6,797,189 B2Enhancement of silicon oxide etch rate and nitride selectivity using hexafluorobutadiene or other heavy perfluorocarbon200412
US 6,838,388 B2Fabrication method of semiconductor integrated circuit device200513
US 6,849,193 B2Highly selective process for etching oxide over nitride using hexafluorobutadiene200523