Abstract

A method for fabricating a metal silicide film is described. After providing a silicon material layer, a metal alloy layer is formed to cover the silicon material layer. A thermal process is performed to form a metal alloy silicide layer in a self-aligned way. A wet etching process is performed by using a cleaning solution including sulfuric acid and hydrogen peroxide to remove the residual metals and unreacted metal alloy.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for fabricating a metal silicide layer, comprising: providing a silicon material layer; forming a metal alloy layer on the silicon material layer, wherein the metal alloy layer contains platinum and nickel; performing a first rapid thermal process (RTP) so as to form a metal alloy silicide layer through reaction of silicon in the silicon material layer with the metal alloy layer; and performing a first etching process on a rotation platen by using a cleaning solution at a lower rotation speed to remove the metal alloy layer that is not fully reacted, wherein the cleaning solution is a