Pattern formation method
Abstract
After formation of an underlayer film and an intermediate layer film, a resist pattern formed by the first pattern exposure with the first resist film and the second pattern exposure with the second resist film is transferred to the intermediate layer film. The underlayer film is etched using an intermediate layer pattern as a mask to form an underlayer film pattern. Herein, the first and second resist films are chemically amplified resist films. The second resist film contains a greater amount of additive which improves the sensitivity of the resist or which improves the alkaline solubility of resist exposed part.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 5.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A pattern formation method, comprising the steps of: (a) forming an underlayer film on a film to be etched; (b) forming an intermediate layer film on the underlayer film; (c) forming a first resist film on the intermediate layer film and performing exposure and development of the first resist film via a first photomask having a first pattern to form a first resist pattern; (d) etching the intermediate layer film using the first resist pattern as a mask to transfer the first resist pattern into the intermediate layer so as to form a first intermediate layer pattern which has the first pattern;
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (2)
- Maenhoudt, M. et al., "Double Patterning scheme for sub-0.25 k1 single damascene structures at NA=0.75, lambda=193nm," Optical Microlithography XVIII, vol. 5754, pp. 1508-1518, Bellingham, WA 2005.
- Maenhoudt, M. et al., "Double Patterning scheme for sub-0.25 k1 single damascene structures at NA=0.75, λ=193nm," Optical Microlithography XVIII, vol. 5754, pp. 1508-1518, Bellingham, WA 2005.