Patents
US 7,943,033 B2#44040155 Most CitedActiveUnited States (USPTO)Utility

Electrolytic copper plating method, pure copper anode for electrolytic copper plating, and semiconductor wafer having low particle adhesion plated with said method and anode

2Forward Citations (#44040155 Global)
0.1/yrCitation Velocity (#41862215 Global)
0.92Citation PageRank (#46826147 Global)
26Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention pertains to an electrolytic copper plating method characterized in employing pure copper as the anode upon performing electrolytic copper plating, and performing electrolytic copper plating with the pure copper anode having a crystal grain diameter of 10 μm or less or 60 μm or more. Provided are an electrolytic copper plating method and a pure copper anode for electrolytic copper plating used in such electrolytic copper plating method capable of suppressing the generation of particles such as sludge produced on the anode side within the plating bath upon performing electrolytic copper plating, and capable of preventing the adhesion of particles to a semiconductor wafer, as well as a semiconductor wafer plated with the foregoing method and anode having low particle adhesion.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An assembly for performing electrolytic copper plating, comprising a plating bath containing a copper sulfate plating liquid and an anode and cathode submerged in said plating liquid within said plating bath, said anode comprising a copper anode having a purity, crystal grain diameter, and oxygen content that enables said copper anode to inhibit generation of sludge during electroplating, said crystal grain diameter being from 100 μm to 2000 μm and said purity of said copper anode being 3N (99.9 wt %) to 6N (99.9999 wt %), excluding gas components.

  2. Claim 2Depends on #1

    An assembly according to claim 1 , wherein said crystal grain diameter of said copper anode is 100 μm to 500 μm.

  3. Claim 3Depends on #2

    An assembly according to claim 2 , wherein said cathode is a semiconductor wafer.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (26)

PatentTitleYearCitations
US 2,923,671 ACopper electrodeposition process and anode for use in same196018
US 3,691,031 AMethod of applying a niobium layer to a copper carrier by electrolytic deposition from fused salts197212
US 4,696,729 AElectroplating cell1987160
US 5,147,466 AMethod of cleaning a surface by blasting the fine frozen particles against the surface199236
US 6,113,771 AElectro deposition chemistry2000116
JP 2001240949 AMethod of manufacturing for worked billet of high- purity copper having fine crystal grain—38
US 2002000371 A1Substrate processing apparatus and substrate plating apparatus—30
US 6,372,119 B1Inert anode containing oxides of nickel iron and cobalt useful for the electrolytic production of metals200255
US 6,451,135 B1High-purity copper sputtering targets and thin films200245
US 2003029527 A1Phosphorized copper anode for electroplating—13
US 6,527,920 B1Copper electroplating apparatus2003154
US 6,531,039 B2Anode for plating a semiconductor wafer200314
US 6,562,222 B1Copper electroplating liquid, pretreatment liquid for copper electroplating and method of copper electroplating200334
US 2003188975 A1Copper anode for semiconductor interconnects—16
US 2004007474 A1Electrolytic copper plating method, phosphorous copper anode for electrolytic plating method, and semiconductor wafer having low particle adhesion plated with said method and anode—10
US 2004149588 A1Electrolytic cooper plating method, phosphorus-containing anode for electrolytic cooper plating, and semiconductor wafer plated using them and having few particles adhering to it—14
US 2004200727 A1Copper electroplating method, pure copper anode for copper electroplating, and semiconductor wafer plated thereby with little particle adhesion—19
US 6,821,407 B1Anode and anode chamber for copper electroplating200457
US 6,830,673 B2Anode assembly and method of reducing sludge formation during electroplating200416
US 7,138,040 B2Electrolytic copper plating method, phosphorous copper anode for electrolytic plating method, and semiconductor wafer having low particle adhesion plated with said method and anode200612
US 7,374,651 B2Electrolytic copper plating method, phosphorus-containing anode for electrolytic copper plating, and semiconductor wafer plated using them and having few particles adhering to it20089
US 2008210568 A1Electrolytic Copper Plating Method, Phosphorous Copper Anode for Electrolytic Copper Plating, and Semiconductor Wafer having Low Particle Adhesion Plated with said Method and Anode—8
US 2010000871 A1Electrolytic Copper Plating Method, Pure Copper Anode for Electrolytic Copper Plating, and Semiconductor Wafer having Low Particle Adhesion Plated with said Method and Anode—3
US 7,648,621 B2Copper electroplating method, pure copper anode for copper electroplating, and semiconductor wafer plated thereby with little particle adhesion20104
US 2010096271 A1Copper Anode or Phosphorous-Containing Copper Anode, Method of Electroplating Copper on Semiconductor Wafer, and Semiconductor Wafer with Low Particle Adhesion—3
US 7,799,188 B2Electrolytic copper plating method, pure copper anode for electrolytic copper plating, and semiconductor wafer having low particle adhesion plated with said method and anode20106

Non-Patent Literature (2)

  • Lamontagne et al., "Effect of Oxygen on the Cu-Cu2Se-Ag System", Minerals Engineering, vol. 12, No. 12, pp. 1441-1457, Apr. 1, 1999.
  • Walker, "The Anatomy of a Copper Anode", Plating and Surface Finishing, vol. 77, No. 10., pp. 16-17, Oct. 1990.