Copper alloy sheet and QFN package
Abstract
A QFN package is provided with a lead frame formed by processing a copper alloy sheet containing 0.01 to 0.50% by mass Fe, 0.01 to 0.20% by mass P, and Cu and inevitable impurities as other components, having a micro Vickers hardness of 150 or above, a uniform elongation of 5% or below and a local elongation of 10% or below, or a copper alloy sheet containing 0.05 to 2% by mass Ni, 0.001 to 0.3% by mass P, 0.005 to 5% by mass Zn, and Cu and inevitable impurities as other components, having a micro Vickers hardness of 150 or above, a uniform elongation of 5% or below and a local elongation of 10% or below. Lead burrs formed during the dicing of the QFN package are short, and a dicing blade used for dicing the QFN package is abraded at a low wear-out rate.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 11.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A QFN package comprising a lead frame made by processing a copper alloy sheet of a copper alloy containing 0.01 to 0.50% by mass Fe, 0.01 to 0.20% by mass P, and Cu and inevitable impurities as other components, having a micro Vickers hardness of 150 or above, a uniform elongation of 5% or below and a local elongation of 10% or below.
- Claim 2Depends on #1
The QFN package according to claim 1 , wherein the copper alloy further contains 0.005 to 5% by mass Sn.
- Claim 3Depends on #1
The QFN package according to claim 1 , wherein the copper alloy further contains 0.005 to 3.0% by mass Zn.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (11 of 11 total)
References Cited — Backward Prior Art (18)
Non-Patent Literature (2)
- U.S. Appl. No. 12/374,154, filed Jan. 16, 2009, Aruga, et al.
- U.S. Appl. No. 12/441,904, filed Mar. 19, 2009, Aruga, et al.