Patents
US 7,926,543 B2#61519690 Most CitedActiveUnited States (USPTO)Utility

Method for producing metal/ceramic bonding substrate

1Forward Citations (#61519690 Global)
0.1/yrCitation Velocity (#51280679 Global)
0.75Citation PageRank (#61519690 Global)
9Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

After a molten metal of aluminum or an aluminum alloy having a temperature, which is higher than the liquidus line temperature of aluminum or the aluminum alloy by 5 to 200° C., is injected into a mold, when the mold is cooled to solidify the molten metal, the molten metal injected into the mold is pressurized at a pressure of 1.0 to 100 kPa from a high-temperature side to a low-temperature side, and the mean cooling rate is set to be 5 to 100° C./minute while the mold is cooled from the liquidus line temperature to 450° C., the temperature gradient formed in the mold being set to be in the range of from 1° C./cm to 50° C./cm.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing a metal/ceramic bonding substrate, the method comprising the steps of: setting a ceramic substrate in a porous carbon mold having an inlet; injecting a molten metal of aluminum or an aluminum alloy into the mold from the inlet so as to allow the molten metal to contact the ceramic substrate; cooling the opposite side of the mold to the inlet to form a temperature gradient of 1 to 50° C./cm in the mold to cool and solidify the molten metal to bond one side of a metal plate of aluminum or the aluminum alloy to one side of the ceramic substrate, the molten metal being coole

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)