Patents
US 7,923,281 B2#14926923 Most CitedActiveUnited States (USPTO)Utility

Roll-to-roll processing method and tools for electroless deposition of thin layers

7Forward Citations (#14926923 Global)
0.5/yrCitation Velocity (#17569700 Global)
1.93Citation PageRank (#15400304 Global)
20Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A deposition method and a system are provided to deposit a CdS buffer layer on a surface of a solar cell absorber layer of a flexible workpiece from a process solution including all chemical components of the CdS buffer layer material. CdS is deposited from the deposition solution while the flexible workpiece is heated and elastically shaped by a heated shaping plate to retain the process solution on the solar cell absorber layer. The flexible workpiece is elastically shaped by pulling a back surface of the flexible workpiece into a cavity area in the heated shaping plate using an attractive force.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 7.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of depositing a buffer layer material from a solution to an exposed surface of a solar cell absorber layer disposed on a continuous flexible workpiece for manufacturing solar cells as the continuous flexible workpiece is advanced through a roll-to-roll system, comprising: advancing a section of the continuous flexible workpiece from a supply roll and having a flat shape onto a heated plate including a cavity area, wherein the cavity area of the heated plate is configured to elastically alter the section of the continuous flexible workpiece into a curved shape that conforms to the cavi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 4,798,660 AMethod for forming Cu In Se2 films1989284
US 4,915,745 AThin film solar cell and method of making1990256
US 5,410,796 ACopper/copper alloy and graphite fiber composite and method199551
US 5,476,811 AMethod of growing epitaxial layers199535
US 5,997,956 AChemical vapor deposition and powder formation using thermal spray with near supercritical and supercritical fluid solutions199992
US 6,048,442 AMethod for producing thin-film solar cell and equipment for producing the same2000153
US 6,092,669 AEquipment for producing thin-film solar cell2000136
US 2001006734 A1Heat treatable coated glass—24
US 6,537,845 B1Chemical surface deposition of ultra-thin semiconductors2003124
US 6,547,876 B2Apparatus for growing epitaxial layers on wafers by chemical vapor deposition200325
US 6,923,625 B2Method of forming a reactive material and article formed thereby2005103
US 7,541,067 B2Method and apparatus for continuous processing of buffer layers for group IBIIIAVIA solar cells200915
US 2009162969 A1Method and apparatus to form solar cell absorber layers with planar surface—24
US 7,585,547 B2Method and apparatus to form thin layers of materials on a base200911
US 2009246908 A1Roll-to-roll processing method and tools for electroless deposition of thin layers—22
US 2009255461 A1Apparatus for Simultaneous Roll-to-Roll Wet Processing of Two Workpieces Disposed Within a Single Chamber—12
US 2010087015 A1Feedback for buffer layer deposition—9
US 2010086699 A1Solution containment during buffer layer deposition—11
US 2010291727 A1Roll-to-roll processing method and tools for electroless deposition of thin layers—14