Patents
US 7,923,063 B2#109595220 Most CitedActiveUnited States (USPTO)Utility

Method of making glass including surface treatment with aluminum chloride using combustion deposition prior to deposition of antireflective coating

0Forward Citations (#109595220 Global)
0.0/yrCitation Velocity (#109595220 Global)
0.56Citation PageRank (#109595220 Global)
33Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

This invention relates to a method of making glass. In certain example embodiments, a major surface(s) of the glass is treated with aluminum chloride (e.g., AlCl 3 ). This treating, or application of an aluminum chloride based layer on the glass substrate, may be performed using combustion deposition. The combustion deposition may be performed at or just prior to the annealing lehr in certain example embodiments, or at any other suitable location. The aluminum chloride barrier layer, applied at a desirable glass temperature, helps to reduce sodium leaching or diffusion from the glass during conditions such as high heat and/or humidity, thereby improving the durability and/or stability of the resulting product.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 33 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of making a coated article, the method comprising: providing soda-lime-silica based glass comprising a base glass portion that includes: Ingredient wt. % SiO 2 67-75% Na 2 O 10-20% CaO 5-15% Al 2 O 3 0-7% K 2 O

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (33)

PatentTitleYearCitations
GB 835,820 AMethod of treating glass articles—13
DE 2,160,723 A1Mechanically strong glass vessel - produced by surface treatment—4
US 4,228,206 AMethod of processing glass tubing198024
SU 988,787 A1Method for improving chemical resistance of glass19836
JP S60176952 AMethod for preventing weathering of glass—11
US 5,054,355 AAutomatic glass cutting and positioning system199130
US 5,510,144 AProcess for preventing heavy metal migration in crystal articles199614
US 5,652,021 ACombustion chemical vapor deposition of films and coatings1997120
US 5,782,949 ADevice for the manufacture of flat glass sheet with improved characteristics199812
US 5,858,465 ACombustion chemical vapor deposition of phosphate films and coatings199969
JP H11228172 APlasma corrosion resistant glass and device using the same—26
US 5,948,132 AGlass sheet strip annealing method199911
US 6,013,318 AMethod for the combustion chemical vapor deposition of films and coatings200076
US 6,193,911 B1Precursor solution compositions for electronic devices using CCVD200154
US 6,602,371 B2Method of making a curved vehicle windshield200363
US 6,711,917 B2Photochromic float glasses and methods of making the same20049
US 6,713,178 B2Highly tetrahedral amorphous carbon coating on glass200446
US 6,716,780 B2Grey glass composition including erbium, holmium, and/or yttrium200482
US 6,796,146 B2Method for manufacturing patterned glass products200458
WO 2004/096724 A1Alkaline glasses with modified surfaces and method for producing same—22
US 6,853,433 B2Liquid crystal display device having soda-lime glass and method of fabricating the same20058
WO 2005/087678 A1Process for the deposition of aluminium oxide coatings—3
US 6,949,484 B2Clear glass composition200537
US 6,953,759 B2Glass composition with low visible and IR transmission200517
US 2007030569 A1Broad band antireflection coating and method of making same—61
US 2007031655 A1Transparent articles with anti-reflective coating and methods of making the same—2
US 2007116966 A1Solar cell with antireflective coating with graded layer including mixture of titanium oxide and silicon oxide—53
US 2007113881 A1Method of making solar cell with antireflective coating using combustion chemical vapor deposition (CCVD) and corresponding product—70
US 2007141349 A1Alkaline glasses with modified glass surfaces and process for the production thereof—12
US 2007178316 A1First surface mirror with sol-gel applied protective coating for use in solar collector or the like—46

Non-Patent Literature (5)

  • "Combustion Chemical Vapor Deposition: A Novel Thin-Film Deposition Technique", Hunt et al., 1993 American Institute of Physics, Apr. 21, 1993.
  • "Growth of Thin Films of Molybdenum and Tungsten Oxides by Combustion CVD using Aqueous Precursor Solutions", Davis et al., Chemical Vapor Deposition 2004, 10, No. 1, pp. 29-34.
  • International Search Report dated Feb. 12, 2009.
  • U.S. Appl. No. 11/492,204, filed Jul. 25, 2006.
  • U.S. Appl. No. 11/878,318, filed Jul. 23, 2007.