Patents
US 7,919,343 B2#30301712 Most CitedActiveUnited States (USPTO)Utility

Group III nitride crystal and method for surface treatment thereof, group III nitride stack and manufacturing method thereof, and group III nitride semiconductor device and manufacturing method thereof

3Forward Citations (#30301712 Global)
0.2/yrCitation Velocity (#32885387 Global)
1.23Citation PageRank (#30940029 Global)
10Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method for surface treatment of a group III nitride crystal includes the steps of lapping a surface of a group III nitride crystal using a hard abrasive grain with a Mohs hardness higher than 7, and abrasive-grain-free polishing the lapped surface of the group III nitride crystal using a polishing solution without containing abrasive grain, and the polishing solution without containing abrasive grain has a pH of not less than 1 and not more than 6, or not less than 8.5 and not more than 14. Accordingly, the method for surface treatment of a group III nitride crystal can be provided according to which hard abrasive grains remaining at the lapped crystal can be removed to reduce impurities at the crystal surface.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for surface treatment of a group III nitride crystal, comprising the steps of: lapping a surface of a group III nitride crystal using a hard abrasive grain with a Mohs hardness higher than 7; and abrasive-grain-free polishing for polishing said lapped surface of said group III nitride crystal using a polishing solution without containing abrasive grain, said polishing solution without containing abrasive grain having a pH of not less than 1 and not more than 6, or not less than 8.5 and not more than 14.

  2. Claim 2Depends on #1

    The method for surface treatment of a group III nitride crystal according to claim 1 , wherein in said step of abrasive-grain-free polishing, polishing is performed using a polishing pad with a compressibility of not less than 1.5% and not more than 20% and at a polishing pressure of not less than 0.98 kPa and not more than 58.8 kPa.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (10)

PatentTitleYearCitations
US 6,399,500 B1Mechano-chemical polishing of crystals and epitaxial layers of GaN and Ga1-x-yA1xInyN200230
JP 2003165799 AGallium nitride single crystal substrate, method for growing the same and method for producing the same—64
JP 2003183100 ASingle crystal gallium nitride substrate, crystal growth method for single crystal gallium nitride, and production method for single crystal gallium nitride substrate—87
US 2007254401 A1Method of processing a surface of group III nitride crystal and group III nitride crystal substrate—10
US 2008012025 A1GaN crystal substrate, fabricating method of GaN crystal substrate, and light-emitting device—9
US 2008057608 A1Manufacturing method of group III nitride substrate, group III nitride substrate, group III nitride substrate with epitaxial layer, manufacturing method of group III nitride substrate with epitaxial layer, and manufacturing method of group III nitride device—24
US 7,416,604 B2Nitride crystal, nitride crystal substrate, epilayer-containing nitride crystal substrate, semiconductor device and method of manufacturing the same200832
US 7,662,239 B2Method of producing group 3 nitride substrate wafers and group 3 nitride substrate wafers20103
US 2010210089 A1SUBSTRATE HAVING THIN FILM OF GaN JOINED THEREON AND METHOD OF FABRICATING THE SAME, AND A GaN-BASED SEMICONDUCTOR DEVICE AND METHOD OF FABRICATING THE SAME—21
US 2010224963 A1Compound semiconductor substrate, semiconductor device, and processes for producing them—16