Patents
US 7,915,474 B2#57223187 Most CitedActiveUnited States (USPTO)Utility

Aqueous phase oxidation process

1Forward Citations (#57223187 Global)
0.1/yrCitation Velocity (#51091017 Global)
0.79Citation PageRank (#57223187 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An improved oxidization process may be used to oxidize a wide variety of feedstocks. Oxidation takes place in a reactor where the feedstock is mixed with an oxidizing acid, such as nitric acid. The reaction mixture may also include a secondary oxidizing acid such as sulfuric acid as well as water and/or dissolved and mechanically mixed oxygen gas. The reactor may be maintained at an elevated pressure such as at least approximately 2070 kPa or desirably at least approximately 2800 kPa. The temperature of the reaction mixture may be maintained at no more than 210° C. In the various embodiments described herein, the process may include: combining recycled effluent from the reactor with the feedstock, combining one or more oxidizing acids with the feedstock, comminuting the feedstock to reduce the size of the particles, feeding the feedstock into the high pressure reactor at an approximately constant feed rate, dispersing oxygen gas from the headspace of the reactor into the reaction mixture, and/or removing all or almost all of the gas from the reactor through the liquid effluent.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method comprising: feeding a feedstock into a reactor at a feed rate that is approximately constant; oxidizing the feedstock in the reactor, the feedstock being part of a reaction mixture that also includes nitric acid and a secondary oxidizing acid; and maintaining a pressure in the reactor of at least approximately 2070 kPa; wherein the feed rate is approximately constant even though the pressure in the reactor may vary from approximately 2070 kPa to 6,900 kPa; and wherein the reaction mixture, excluding solids, includes no more than 5 wt % of the secondary oxidizing acid.

  2. Claim 2Depends on #1

    The method of claim 1 wherein the feedstock is a slurry.

  3. Claim 3Depends on #2

    The method of claim 2 wherein the slurry includes nitric acid and/or the secondary oxidizing acid.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

PatentTitleYearCitations
US 9,272,936 B2Waste treatment process20161

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,637,371 ADirect pressure leaching of copper-iron sulphides197261
US 3,649,665 AHydrocarbon oxidation with nitric oxide and oxygen197213
US 3,793,429 ANitric acid process for recovering metal values from sulfide ore materials containing iron sulfides197460
GB 1,407,520 AElectrolytic hydrometallurgical process to recover copper from sulphide ore concentrates—7
US 3,939,280 AProcess for treating animal waste197693
US 3,953,577 AProcess for purifying gases containing HCN197617
US 3,960,718 AMethod and apparatus for treating liquid sewage and waste197661
US 4,045,279 AProcess for the manufacture of pulp using sodium carbonate and oxygen197733
US 4,076,579 APulping of lignocellulosic material by sequential treatment thereof with nitric oxide and oxygen197835
US 4,081,366 AProcess for dewatering organic waste product197844
US 4,084,961 ATreatment of metal bearing mineral material197829
US 4,132,636 AMethod for treating gas liquor197930
US 4,141,829 AProcess for wet oxidation of organic substances197968
US 4,193,970 AProcess for the precipitation of iron as jarosite198018
US 4,235,858 AProcesses for producing nitric acid by utilization of cold oxygen198025
US 4,239,613 ADeashed coal from nitric acid oxidation of aqueous coal slurry198015
US 4,272,383 AMethod and apparatus for effecting subsurface, controlled, accelerated chemical reactions1981136
GB 1,591,274 AMethod for treating gas liquor—8
US 4,606,763 AProcess for the pressure oxidation acid leaching of non-ferrous metal and iron-containing sulphidic material198648
US 4,647,307 AProcess for recovering gold and silver from refractory ores198745
US 4,692,252 AMethod of removing scale from wet oxidation treatment apparatus198741
US 4,744,908 AProcess for effecting chemical reactions198825
EP 0,119,685 B1Hydrometallurgical arsenopyrite process19887
US 4,793,919 AWet oxidation system198832
US 4,803,054 AAsymmetric heat-exchange reaction apparatus for effecting chemical reactions198944
US 4,849,025 ADecoking hydrocarbon reactors by wet oxidation198935
US 4,878,945 AHydrometallurgical process for treating refractory ores containing precious metals198931
US 4,891,139 AMethod for wet oxidation treatment199023
US 4,897,156 AProcess for activating cellulose pulp with NO and/or NO2 and oxygen in the presence of nitric acid and then delignifying bleaching the activated cellulose pulp199021

Non-Patent Literature (3)

  • Information about Related Patents and Patent Applications, see the section of the accompanying Information Disclosure Statement Letter entitled "Related Patents and Patent Applications" for further information.
  • International Search Report and Written Opinion, PCT/US2010/028340, Dec. 8, 2010 (12 pgs.).
  • Invitation to Pay Additional Fees, PCT/US2010/028340, Jun. 25, 2010 (6 pgs.).