Patents
US 7,914,899 B2#33127248 Most CitedActiveUnited States (USPTO)Utility

Electrical insulation film

3Forward Citations (#33127248 Global)
0.2/yrCitation Velocity (#33098001 Global)
1.06Citation PageRank (#38537654 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Certain embodiments of the present technology provide a capacitor film comprising a polypropylene material. The capacitor film comprises xylene solubles of at least 0.5 percent by weight. In certain embodiments the xylene solubles are in a range of 0.5 to 1.5 percent by weight. The film also comprises a crystalline fraction melting in the temperature range of 200° C. to 105° C. determined by stepwise isothermal segregation technique. The crystalline fraction comprises a part, the part representing at least 10 percent by weight of said crystalline fraction, and wherein the part melts at a melting rate of 10° C./min. Certain embodiments present a capacitor film where the part melts at or below 140° C. In other embodiments, the said part melts at or below the temperature T=Tm−3° C., wherein Tm is the melting temperature of the capacitor film and/or the polypropylene material, and the part represents at least 45 percent by weight of the crystalline fraction.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An electrical insulation film comprising a polypropylene material, at least one of the electrical insulation film and the polypropylene material comprising: a) xylene solubles in the range of about 0.5 percent to about 1.5 percent by weight; and b) a crystalline fraction crystallizing in the temperature range of 200 to 105° C. determined by stepwise isothermal segregation technique, said crystalline fraction comprising a part; wherein, during subsequent melting at a melting rate of 10° C./min, said part melts at or below 140° C. and said part represents at least 10 percent by weight of said cr

  2. Claim 2Depends on #1

    The electrical insulation film of claim 1 , wherein the film has a strain hardening index of at least 0.15 measured at a deformation rate of 1.00 s −1 at a temperature of 180° C., f

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (3 of 3 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
DE 2,827,764 A1Verfahren zur herstellung eines fuer siegelfaehige folien geeigneten polypropylens—5
EP 0,036,457 A1A method of producing a polypropylene film for electrical appliances—9
US 4,304,890 AMethod for producing propylene copolymers using a catalyst activated prior to copolymerization198127
US 4,404,342 AProcess for preparing a copolymer198324
DD 203,915 A1Verschaeumbare polyaethylen-formmassen—6
US 4,483,971 AProcess for producing terpolymers of propylene, ethylene and another .alpha.198432
DE 3,539,352 A1Polypropylenschaumteilchen—24
EP 0,190,889 A2Polypropylene with free-end long chain branching, process for making it, and use thereof—104
US 4,634,745 ATerpolymer production198724
US 4,701,432 ASupported polymerization catalyst1987561
US 4,705,828 APolypropylene resin composition and biaxially stretched film thereof19878
US 4,808,561 ASupported polymerization catalyst19891,073
EP 0,384,431 A2Process for making a propylene polymer with free-end long chain branching and use thereof—74
EP 0,395,204 A1Metallized oriented polypropylene film with improved metal fracture resistance—6
WO 9,212,182 A1Multi-stage process for producing polyethylene—1,029
US 5,250,631 APolymer compositions199353
US 5,326,625 ASealable, opaque, biaxially orientated multilayer polypropylene film, process for its production and its use199482
WO 9,428,034 A1Supported metallocene catalyst systems for the polymerization of olefins, preparation and use thereof—129
EP 0,674,325 A2Electrically insulating polymer composition and wire or cable using the same—18
EP 0,674,991 A1Crystalline propylene copolymer compositions having a low seal temperature and good ink adhesion—56
WO 9,530,708 A1Applications of isotactic polypropylene, processes and products thereof—41
EP 0,690,458 A2Insulating composition and formed article thereof—26
EP 0,745,637 A1Biaxially oriented film of polypropylene with high area modules—10
EP 0,747,212 A1Biaxially oriented polypropylene film with improved barrier properties against water-vapour and oxygen—15
WO 9,722,633 A1Procatalyst, procatalyst precursor, and process for the preparation of a multimodal ethylene polymer—43
WO 9,810,016 A1Improved propylene polymers for oriented films—42
EP 0,873,862 A2Co-extruded or co-injected laminate comprising at least one propylene graft copolymer layer—18

Non-Patent Literature (5)

  • Cazenave, J., et al., Short-term mechanical and structural approaches for the evaluation of polyethylene stress crack resistance Groupe d'Etude de Metallurgie Physique et de Physique des Materiaux, Polymer 47, pp. 3904-3914 (2006).
  • Chujo, R. Heptad configurational analysis of 13C N.M.R. spectra in highly isotactic polypropylene, Polymer 29, vol. 29, January, pp. 138-143 (1988).
  • Chujo, R., Two-site model analysis of 13C n.m.r, of polypropylene polymerized by Ziegler-Natta catalyst with external alkoxysilane donors, Polymer, vol. 35, part II, pp. 339-342 (1994).
  • Ed. J. Sheirs, W. Kaminski, "Metallocenebased Polyolefines" vol. 1 (1999) 401-424.
  • Gahleitner, Markus et al., "Propylene-Ethylene Random Copolymers: Comonomer Effects on Crystallinity and Application Properties," Journal of Applied Polymer Science, 95(5), pp. 1073-1081, (2005).