Gas-barrier laminate
Abstract
A gas-barrier laminate with a plastic substrate, an inorganic thin film formed on at least one surface of the plastic substrate, and a coating layer formed by applying a coating material on a surface of the inorganic thin film, wherein said coating layer contains a polyester-based resin having a molecular weight of 3000 to 15000 and a polyurethane-based resin having a molecular weight of 8000 to 30000 at a weight ratio of 5/95 to 95/5, and said gas-barrier laminate has an oxygen permeability of not more than 25 fmol/m 2 /s/Pa; and a gas-barrier laminate comprising a plastic substrate, an inorganic thin film formed on at least one surface of the plastic substrate, and a coating layer formed by applying a coating material on a surface of the inorganic thin film, wherein the gas-barrier laminate exhibits an oxygen permeability of not more than 50 fmol/m 2 /s/Pa as measured with respect to a gas-barrier film obtained by laminating an unstretched polypropylene film having a thickness of 60 μm on the coating layer of the gas-barrier laminate after subjecting the gas-barrier film to hydrothermal treatment at 120° C. for 30 min, and the coating layer has either a hardness of 0.1 to 0.5 GPa
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 7.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A gas-barrier laminate, comprising: a plastic substrate; an inorganic thin film formed on at least one surface of the plastic substrate; and a coating layer on a surface of the inorganic thin film; wherein the coating layer comprises: a polyester resin having a molecular weight of 3000 to 15000, and a polyurethane resin having a molecular weight of 8000 to 3000, a weight ratio of the polyester resin to the polyurethane resin is from 5/95 to 95/5, and an oxygen permeability of the gas-barrier laminate is not more than 25 fmol/m 2 /s/Pa.
- Claim 2Depends on #1
The gas-barrier laminate according to claim 1 , wherein the polyester-based resin and the polyurethane-based resin respectively have a glass transition temperature of 55 to 100° C. and an acid value of 1 to 100 mg KOH/g.
- Claim 3Depends on #1
The gas-barrier laminate according to claim 1 , wherein the coating
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (7 of 7 total)
References Cited — Backward Prior Art (16)
Non-Patent Literature (2)
- International Preliminary Report on Patentability dated Mar. 23, 2005 issued for corresponding International Patent Application No. PCT/JP2005/005189.
- International Search Report dated Jul. 12, 2005 issued for corresponding International Patent Application No. PCT/JP2005/005189.