Patents
US 7,910,165 B2#30203618 Most CitedExpiredUnited States (USPTO)Utility

Ruthenium layer formation for copper film deposition

3Forward Citations (#30203618 Global)
0.2/yrCitation Velocity (#32879538 Global)
1.24Citation PageRank (#30682825 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method of ruthenium layer formation for high aspect ratios, interconnect features is described. The ruthenium layer is formed using a cyclical deposition process. The invention generally provides a method of forming a film on a substrate surface including positioning a substrate within a process chamber, exposing a ruthenium-containing compound to the substrate surface, purging the process chamber with a purge gas, reducing the ruthenium-containing compound with a reductant to form a ruthenium layer on the substrate surface and purging the process chamber with the purge gas. The ruthenium-containing compound is selected from the group consisting of bis(dialkylpentadienyl)ruthenium compounds, bis(alkylpentadienyl) ruthenium compounds, bis(pentadienyl)ruthenium compounds, and combinations thereof.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for forming a ruthenium material on a substrate surface, comprising: positioning a substrate within a process chamber; exposing a ruthenium-containing compound to the substrate while forming a ruthenium-containing compound film thereon, wherein the ruthenium-containing compound is selected from the group consisting of bis(dialkylpentadienyl) ruthenium compounds, bis(alkylpentadienyl) ruthenium compounds, bis(pentadienyl) ruthenium compounds, and combinations thereof; purging the process chamber with a purge gas; exposing a reducing gas comprising ammonia and atomic hydrogen to the rut

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the ruthenium-containing compound comprises at least one alkyl group selected from the g

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 5,372,849 AChemical vapor deposition of iron, ruthenium, and osmium1994170
US 5,933,753 AOpen-bottomed via liner structure and method for fabricating same1999256
US 5,962,716 AMethods for preparing ruthenium and osmium compounds199983
US 6,063,705 APrecursor chemistries for chemical vapor deposition of ruthenium and ruthenium oxide2000208
US 6,114,557 AMethods for preparing ruthenium and osmium compounds200044
JP 2001111000 ASemiconductor element and manufacturing method thereof—104
US 2001006838 A1Methods of forming ruthenium film by changing process conditions during chemical vapor deposition and ruthenium films formed thereby—40
JP 2001237400 AMethod of manufacturing capacitor of semiconductor device—23
WO 0,188,972 A1Process for producing integrated circuits—26
US 2001054730 A1Metal-insulator-metal capacitor and manufacturing method thereof—60
US 2002000587 A1Method for forming capacitor of nonvolatile semiconductor memory device and the capacitor—26
US 2002004293 A1Method of growing electrical conductors—137
US 6,338,991 B1Semiconductor device and method for manufacturing the same200262
US 2002025627 A1RuSixOy-containing adhesion layers and process for fabricating the same—29
US 2002028556 A1RuSixOy-containing adhesion layers and process for fabricating the same—25
US 6,365,502 B1Microelectronic interconnect material with adhesion promotion layer and fabrication method2002111
US 2002076881 A1RuSixOy-containing adhesion layers and process for fabricating the same—17
US 2002074577 A1RuSixOy-containing adhesion layers and process for fabricating the same—17
US 2002081381 A1Atomic layer deposition of cobalt from cobalt metallorganic compounds—93
US 6,423,619 B1Transistor metal gate structure that minimizes non-planarity effects and method of formation200273
US 2002102810 A1Method for fabricating a semiconductor device—44
US 6,440,495 B1Chemical vapor deposition of ruthenium films for metal electrode applications2002127
US 2002121697 A1Process for the formation of RuSixOy-containing barrier layers for high-k dielectrics—26
US 2002125516 A1RuSixOy-containing adhesion layers and process for fabricating the same—22
US 6,462,367 B2RuSixOy-containing adhesion layers200253
US 6,479,100 B2CVD ruthenium seed for CVD ruthenium deposition200255
US 6,482,740 B2Method of growing electrical conductors by reducing metal oxide film with organic compound containing -OH, -CHO, or -COOH2002286

Non-Patent Literature (5)

  • Aaltonen, et al., "Atomic Layer Deposition of Ruthenium from RuCp2 and Oxygen: Film Growth and Reaction Mechanism Studies," Electrochemical Society Proceedings Volume Aug. 2003 pp. 946-953.
  • Aaltonen, et al., "Atomic Layer Deposition of Ruthenium Thin Films from Ru(thd)3 and Oxygen," Chem. Vap. Deposition (2004), 10, No. 4 pp. 215-219.
  • Aaltonen, et al., "Ruthenium Thin Films Grown by Atomic Layer Deposition," Chem. Vap. Deposition (2003), 9, No. 1 pp. 45-49.
  • Aoyama, et al.; "Ruthenium Films Prepared by Liquid Source Chemical Vapor Deposition Using Bis-(ethylcyclopentadienyl)ruthenium," Jpn. J. Appl. Phys. vol. 38 (1999) pp. L1134-L1136.
  • Dadgar, et al., "Growth of Ru doped semi-insulating InP by low pressure metalorganic chemical vapor deposition," Journal of Crystal Growth 195 (1998) pp. 69-73.