Patents
US 7,909,900 B2#39625658 Most CitedActiveUnited States (USPTO)Utility

Method of making a modified abrasive compact

2Forward Citations (#39625658 Global)
0.1/yrCitation Velocity (#41609699 Global)
1.02Citation PageRank (#40486649 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of treating the working surface of an abrasive compact having a working surface. The working surface, or a region adjacent the working surface, of the abrasive compact is contacted with a halogen gas or a gaseous environment containing a source of halide ions, preferably at a temperature at or below 800° C., in order to remove catalysing material and any foreign metal matrix material from the region adjacent the working surface.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of treating an abrasive compact having a working surface, the method comprising contacting the working surface, or a region adjacent the working surface, of the abrasive compact with a halogen gas or a gaseous environment containing a source of halide ions in order to remove catalysing material and any foreign metal matrix material from the region adjacent the working surface.

  2. Claim 2Depends on #1

    A method according to claim 1 , wherein contacting of the working surface or adjacent region takes place at a temperature at or below 800° C.

  3. Claim 3Depends on #1

    A method according to claim 1 , wherein contacting of the working surface or adjacent region takes place at a temperature of from about 300° C. to about 800° C.

Technical Overview & Description