Processes for treating aluminium dross residues
Abstract
There is provided a process for preparing aluminium chloride comprising leaching aluminium dross residues with H 2 SO 4 so as to obtain a leachate; and hydrochlorinating the leachate so as to obtain aluminium chloride. If desired, aluminium chloride can then be converted into alumina.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 1.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for treating aluminium dross residues comprising: leaching aluminium dross residues, at a temperature of at least 200° C., with H 2 SO 4 having a concentration of about 98% so as to obtain a mixture comprising a solid and a liquid, and separating said solid from said liquid; solubilizing in water at least a portion of minerals and metals contained in said solid so as to obtain a leachate; hydrochlorinating said leachate so as to obtain aluminium chloride; and converting said aluminium chloride into alumina, wherein in said process, at least 80% by weight of the Al atoms contained in
- Claim 2Depends on #1
The process of claim 1 , wherein said leaching is carried out at a temperature of at least 225° C.
- Claim 3Depends on #1
The process of claim 1 , wherein said leaching is carried out at a temperature of
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2017009311 A1 | Secondary material for steel refining | — | 2 |