Patents
US 7,902,554 B2#63258202 Most CitedActiveUnited States (USPTO)Utility

Polysilicon film having smooth surface and method of forming the same

0Forward Citations (#63258202 Global)
0.0/yrCitation Velocity (#63258202 Global)
0.56Citation PageRank (#63258202 Global)
10Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method of forming a polysilicon film having smooth surface using a lateral growth and a step-and-repeat laser process. Amorphous silicon formed in a first irradiation region of a substrate is crystallized to form a first polysilicon region by a first laser shot. Then, the substrate is moved a predetermined distance, and irradiated by a second laser shot. The polysilicon region is then recrystallized and locally planarized by subsequent laser shots. After multiple repetitions of the irradiation procedure, the amorphous silicon film formed on a substrate is completely transformed into a polysilicon film. The polysilicon film includes lateral growth crystal grains and nano-trenches formed in parallel on the surface of the polysilicon film. A longitudinal direction of the nano-trenches is substantially perpendicular to a lateral growth direction of the crystal grains.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A polysilicon layer formed on a substrate, comprising: a plurality of lateral growth crystal grains arranged in parallel with a plurality of grain boundaries therebetween and extended in a grain direction, each of the lateral growth crystal grains including a plurality of nano-trenches formed on a top surface of the lateral growth crystal grains, a longitudinal direction of the nano-trenches substantially perpendicular to the grain direction of the lateral growth crystal grains, wherein the nano-trenches have a depth smaller than about 20 nm, and a distance D between two adjacent nano-trenches

  2. Claim 2Depends on #1

    The polysilicon layer according to claim 1 , wherein the surface of the polysilicon layer has a root-mean-square (RMS) roughness no greater than 5 nm.

  3. Claim 3Independent Claim

    A polysilicon layer formed on a substrate, comprising: a p

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.