Method of producing a semiconductor device with an aluminum or aluminum alloy rear electrode
Abstract
A method of producing a semiconductor device having a thickness of 90 μm to 200 μm and with an electrode on the rear surface, which achieves a high proportion of non-defective devices by optimizing the silicon concentration and thickness of the aluminum-silicon electrode. A surface device structure is formed on a first major surface of a silicon substrate. A buffer layer and a collector layer are formed on the second major surface after grinding to reduce the thickness of the substrate. On the collector layer, a collector electrode is formed including a first layer of an aluminum-silicon film having a thickness of 0.3 μm to 1.0 μm and a silicon concentration of 0.5 percent to 2 percent by weight, preferably not more than 1 percent by weight.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of producing a semiconductor device that has a front surface device structure in a region of a first major surface of a silicon substrate and a rear electrode in a region of a second major surface of the silicon substrate, the method comprising the step of: forming an aluminum-silicon film in contact with the second major surface as the rear electrode, wherein the semiconductor device is a reverse blocking type insulated gate bipolar transistor that includes, between the first major surface and the second major surface, a drift layer of a first conductivity type, and a collector layer
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗