Low cost, environmentally favorable, chromium plate replacement coating for improved wear performance

9Forward Citations (#12209045 Global)
0.6/yrCitation Velocity (#13139125 Global)
1.54Citation PageRank (#21887752 Global)
21Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A coating which improves the wear performance of a part is described. The coating is applied over an article such as a part or a workpiece using an electroplating process. The coating broadly includes a cobalt material matrix with a hardness of at least 550 HV and a plurality of carbide particles distributed throughout the cobalt material matrix. The cobalt material matrix may be a cobalt-phosphorous alloy. The particles interspersed throughout the matrix may be chrome carbide or silicon carbide particles.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 9.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A coating for improving the wear performance of an article, said coating comprising: a cobalt material matrix with a hardness in the range of 550 to 1000 HV; said cobalt material matrix consisting of a cobalt phosphorous alloy; said phosphorous in the final coating being present in an amount of from 4.0 to 6.0 wt %; and a plurality of carbide particles selected from the group consisting of chrome carbide particles and silicon carbide particles throughout the cobalt material matrix, said carbide particles having an average particle size in the range of from 2.0 to 10 microns.

  2. Claim 2Depends on #1

    The coating of claim 1 , wherein said carbide particles are present in an amount in the range of from 15 to 30 vol %.

  3. Claim 3Depends on #1

    The coating of claim 1 , wherein said matrix has a hardness in the range of from 550 to 650 HV.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
US 2,594,933 AProcess for electrodepositing hard nickel plate19529
US 2,643,221 AElectrodeposition of phosphorusnickel and phosphorus-cobalt alloys195367
US 3,152,974 AElectroplating magnetic cobalt alloys19649
US 3,753,667 AArticles having electroless metal coatings incorporating wear-resisting particles therein197369
US 4,153,453 AComposite electrodeposits and alloys197929
US 4,305,792 AProcesses for the electrodeposition of composite coatings198153
US 4,528,070 AOrifice plate constructions198560
US 4,673,468 ACommercial nickel phosphorus electroplating198746
JP S63282295 AWear resistant surface layer—14
US 5,154,816 AProcess for depositing an anti-wear coating on titanium based substrates199216
JP H0693469 AMethod for depositing wear resisting coating on titanium based substrate—3
US 5,558,758 AElectrodeposited composite coatings199624
US 5,881,972 AElectroformed sheath and airfoiled component construction199971
US 5,966,585 ATitanium carbide/tungsten boride coatings199938
US 6,040,551 AApparatus for hardening the inside contour of a gun barrel with laser radiation200012
US 6,067,784 AHard facing for cutting edges of agricultural machine blades200034
WO 2004/001100 A1Process for electroplating metallic and metall matrix composite foils, coatings and microcomponents—42
US 2005112399 A1Erosion resistant coatings and methods thereof—45
JP 2005530926 A金属および金属マトリックス複合体箔、コーティング、ならびに超小型部品を電気メッキするためのプロセス—15
WO 2007/021332 A2Composite electroless plating—3
US 2007170068 A1Electrocomposite coatings for hard chrome replacement—13

Non-Patent Literature (1)

  • Japanese Office Action dated Aug. 3, 2009.