Abstract

A method is set forth of forming an ohmic electrode having good characteristics on a SiC semiconductor layer. In the method, a Ti-layer and an Al-layer are formed on a surface of the SiC substrate. The SiC substrate having the Ti-layer and the Al-layer is maintained at a temperature that is higher than or equal to a first temperature and lower than a second temperature until all Ti in the Ti-layer has reacted with Al. The first temperature is the minimum temperature of a temperature zone at which the Ti reacts with the Al to form Al 3 Ti, and the second temperature is the minimum temperature of a temperature zone at which the Al 3 Ti reacts with SiC to form Ti 3 SiC 2 . As a result of this maintaining of temperature step, an Al 3 Ti-layer is formed on the surface of the SiC substrate. The method also comprises further heating the SiC substrate having the Al 3 Ti-layer to a temperature that is higher than the second temperature. As a result of this step of further heating the SiC substrate reacts with Al 3 Ti of the Al 3 Ti-layer to form a Ti 3 SiC 2 -layer on the surface of the SiC substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 5.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a semiconductor device comprising a SiC substrate and an electrode formed on the SiC substrate, the method comprising: forming a Ti-layer on a surface of the SiC substrate; forming an Al-layer on a surface of the Ti-layer; maintaining the SiC substrate having the Ti-layer and the Al-layer at a temperature that is higher than or equal to a first temperature which is the minimum temperature of a temperature zone at which the Ti reacts with the Al to form Al 3 Ti, and lower than a second temperature which is the minimum temperature of a temperature zone at which the Al 3

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • B. Johnson et al., "Mechanism of Ohmic Behavior of AI/Ti Contacts to p-Type 4H-SiC After Annealing," Journal of Applied Physics, vol. 95, No. 10, pp. 5616-5620 (2004).
  • B. Pécz et al., "Ti3SiC2 Formed in Annealed AI/Ti Contacts to p-Type SiC," Applied Surface Science, vol. 206, pp. 8-11 (2003).
  • Crofton et al., Titanium and Aluminum-Titanium Ohmic Contacts to p-Type SiC., Solid State Electronics, vol. 41 (11), pp. 1725-1729 (1997).
  • G. Hui et al., "Ti-AI Based Ohmic Contacts to n-Type 6H-SiC with P+ Ion Implantation," Chinese Physics, vol. 15, No. 9, pp. 2142-2145 (2006).