Impact resistant polyolefin compositions
Abstract
The present invention provides polyolefin composition comprising a 50-80 wt % of propylene homopolymer or copolymer and a first and a second ethylene/alpha-olefin copolymer, said composition having good stress whitening resistance and gloss, in combination with a good balance of mechanical properties.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 48 · Forward citations: 15.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A polyolefin composition comprising (percentages based on the sum of component (A) to (C)): (A) from 50 to 80 wt % of a propylene polymer comprising a polydispersity index value ranging from 4.5 to 10 and a content of isotactic pentads, measured by 13 C-NMR on a fraction insoluble in xylene at 25° C., higher than 97.5 mol %, said polymer being selected from propylene homopolymers or copolymers of propylene with at least one linear or branched alpha-olefin comprising from 2 to 8 carbon atoms other than propylene, said copolymer containing at least 95 wt % (based on the copolymer) of units deri
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 15 total)
References Cited — Backward Prior Art (48)
Non-Patent Literature (2)
- R. Chûjô et al., "Two-site model analysis of 13C n.m.r. of polypropylene polymerized by Ziegler-Natta catalyst with external alkoxysilane donors," Polymer, vol. 35(2), p. 339-342 (1994).
- Y. Inoue et al., "Studies of the stereospecific polymerization mechanism of polypropylene by a modified Ziegler-Natta catalyst based on 125 MHz 13C n.m.r. spectra," Polymer, vol. 25, p. 1640-1644 (1984).